Modulation in current density of metal/n-SiC contact by inserting Al2O3 interfacial layer
نویسندگان
چکیده
Metal contact to SiC is not easy to modulate since the contact can be influenced by the metal, the termination of the SiC, the doping, and the fabrication process. In this work, we introduce a method by inserting a thin Al2O3 layer between metal and SiC to solve this problem simply but effectively. The Al2O3/n-SiC interface composition was obtained with X-ray photoemission spectroscopy, and the electrical properties of subsequently deposited metal contacts were characterized by current-voltage method. We can clearly demonstrate that the insertion of Al2O3 interfacial layer can modulate the current density effectively and realize the transfer between the Schottky contact and ohmic contact.
منابع مشابه
Schottky-barrier height modulation of metal/In0.53Ga0.47As interfaces by insertion of atomic-layer deposited ultrathin Al2O3
The improvement of the metal/InGaAs interface is essential for the future application of InGaAs metal source/drain Schottky-barrier metal-oxide-semiconductor field-effect-transistors. In this article, on In0.53Ga0.47As, the authors examine the recently proposed method of inserting an ultrathin insulator to modulate the effective Schottky-barrier height SBH at the metal/semiconductor interface. ...
متن کاملThe Role of Interface State Density in I-V Characteristics of Metal-Semiconductor Contact With Interfacial Layer
The metal-insulator-semiconductor (MIS) diode is the most useful device in the study of semiconductor surfaces. The current-voltage data of the metal-insulatorsemiconductor Schottky diode are simulated using thermionic emission diffusion equation taking into account the interfacial layer parameters. The calculated current–voltage data are fitted into ideal thermionic emission diffusion equation...
متن کاملA Comparative Corrosion Study of Al/Al2O3-SiC Hybrid Composite Fabricated by Accumulative Roll Bonding (ARB)
In this study, the Al/Al2O3-SiC hybrid composite was produced by accumulative roll bonding (ARB). In the first and the second cycles, the particles were uniformly poured between the Al strips during each ARB cycle. In the subsequent cycles, ARB was repeated up to six cycles without adding the particles between the layers. After the total eight cycles, the particles were distributed uniformly wi...
متن کاملBonding and structure of ceramic-ceramic interfaces.
Quantum molecular dynamics simulations of α-Al2O3(0001)/3C-SiC(111) interfaces reveal profound effects of thermal annealing for producing strong interfaces consisting solely of cation-anion bonds and their consequence on interfacial structures. A Si-terminated SiC surface and Al2O3 form a stronger interface (Si-interface) with a Si-O bond density of 12.2 nm(-2), whereas the C interface has an ...
متن کاملThe effect of powder type and CaO additive on properties of sintered SiC by pressureless sintering in additive system of Al2O3-Y2O3-CaO
In this study, the effect of two types of SiC powders consist of SiC-1 (β-SiC) and SiC-2 (β-SiC+α-SiC) and also different values of CaO additive consist of 0, 0.4 and 0.8 weight percent on sintering behavior of sintered SiC with pressureless technique in Al2O3-Y2O3-CaO additive system was investigated. In all specimens, Al2O3:Y2O3 molar ratio was equal to 3:2 and all amounts of additive were e...
متن کامل