Impact strength of denture base and reline acrylic resins subjected to long-term water immersion.

نویسندگان

  • Amanda Fucci Wady
  • Ana Lucia Machado
  • Carlos Eduardo Vergani
  • Ana Cláudia Pavarina
  • Eunice Teresinha Giampaolo
چکیده

Water may influence the mechanical properties of the acrylic resins. Thus, the effect of water storage on the impact strength (IS) of one denture base (Lucitone 550 - L) and four reline resins (Tokuyama Rebase II - T; UfiGel Hard - U; Kooliner - K; New Truliner - NT) was evaluated. Bars of L were made (60 x 6 x 2 mm) and relined (2 mm) with T, U, K, NT and L. Intact specimens of each material (60 x 6 x 4 mm) were also fabricated for comparative purposes. Specimens were submitted to Charpy impact tests without water storage (control) and after immersion in water for 7, 90 and 180 days. Data (kJ/m(2)) analyzed by two-way ANOVA and Tukey's test (p=0.05) revealed that after 90 days, U exhibited an increase in the IS (0.93) compared to 7 days (0.58). K (1.48) and L/K (7.21) exhibited a decrease at the 7-day period (1.01 and 3.23, respectively). NT (0.60) showed an increase in the IS after 180 days (1.52), whereas L/NT (7.70) showed a decrease (3.17). Water immersion improved the IS of U and NT, and decreased the IS of K, L/K, and L/NT. Water may affect differently the IS of acrylic resins and, consequently, the resistance to fracture of relined denture bases.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Flexural strengths of reinforced denture base resins subjected to long-term water immersion

Objective This study evaluated the flexural strengths of reinforced denture base resins subjected to long-term water immersion. Materials and methods Acrylic denture base resin reinforced with metal wire or glass fiber-reinforced composite (FRC), and without reinforcement were tested. Bar-shaped specimens were fabricated. Half of the specimens were stored in 37 °C distilled water for 50 hours (...

متن کامل

Effect of ethanol solutions as post-polymerization treatment on the properties of acrylic reline resins

Objectives: To evaluate the effect of ethanol solutions as post-polymerization treatment on the shear bond strength and the surface free energy of acrylic reline resins. Methods: Three reline resins (Kooliner, Ufi Gel Hard and Probase Cold) were manipulated and attached to 150 parallelepipeds denture base resin previously aged. Constructed specimens of each resin were randomly divided into cont...

متن کامل

A comparative evaluation of impact strength of conventionally heat cured and high impact heat cured polymethyl methacrylate denture base resins: an in vitro study.

UNLABELLED The denture bases made by using polymethyl methacrylates of Acrylic resin family have excellent physical properties, simple to process and easy to reline, rebase and repair. One of the inherent disadvantages of this material is the liability to break during function. The strength assessment of acrylic resins have been made generally by transverse defection tests. AIM To evaluate th...

متن کامل

Evaluation of adhesion of reline resins to the thermoplastic denture base resin for non-metal clasp denture.

This study aimed to evaluate the tensile and transverse bond strength of chairside reline resins (Tokuyama Rebase II, Mild Rebaron LC) to a thermoplastic acrylic resin (Acrytone) used for non metal clasp denture. The results were compared with those of a conventional heat polymerized acrylic resin (Paladent 20) and a thermoplastic polyamide resin (Biotone). The failure sites were examined by sc...

متن کامل

Impact strength of denture base and reline acrylic resins: An in vitro study

This study evaluated the impact strength of a denture base resin (Lucitone 550-L) and four reline resins (Tokuyama Rebase II-T; Ufi Gel Hard-U; New Truliner-NT, and Kooliner-K), both intact and in a reline combination (L/L, L/T, L/U, L/NT, and L/K). For each group (n = 20), half of the specimens were thermocycled before testing. Charpy tests were performed, and the impact strengths were calcula...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Brazilian dental journal

دوره 22 1  شماره 

صفحات  -