Temperature Threshold and Water Role in CVD Growth of Single-Walled Carbon Nanotubes
نویسندگان
چکیده
An in-depth understanding of the growth process of single-walled carbon nanotubes is of vital importance to the control of the yield of the material and its carbon structure. Using a nickel/silica (Ni/SiOx) catalyst, we have conducted a series of growth experiments with a chemical vapor deposition (CVD) system. We find that there is a temperature threshold in the CVD process, and if the reaction temperature sets above this threshold, there will be no growth of the nanotubes. Moreover, we find that in association with this temperature effect, water plays an important role in the promotion or termination of the growth of single-walled carbon nanotubes.
منابع مشابه
A PARAMETRIC STUDY ON THE GROWTH OF SINGLE-WALLED CARBON NANOTUBES OVER CO-MO/MGO NANOCATALYST IN A FLUIDIZED BED REACTOR BY CCVD METHOD
Single-walled carbon nanotubes (SWNTs) with high yield and quality were synthesized using chemical vapor deposition (CVD) over Co-Mo/ MgO nanocatalyst in a fluidized bed reactor. Different parameters such as temperature, the ratio of hydrocarbon source to hydrogen, the flow rate of gas, growth time, the size of catalyst particles, heating rate, and the kind of hydrocarbon source were examined t...
متن کاملRole of growth temperature in CVD synthesis of Carbon nanotubes from Ni-Co bimetallic catalysts
The effect of temperature variation on the growth of Carbon Nanotubes (CNTs) using Thermal Chemical Vapor Deposition (TCVD) is presented. Nickel and Cobalt (Ni-Co) thin films on Silicon (Si) substrates were used as catalysts in TCVD technique. Acetylene gas was used in CNTs growth process at the controlled temperature ranges from 850-1000 ̊ C. Catalysts and CNTs characterization was carried out ...
متن کاملRole of growth temperature in CVD synthesis of Carbon nanotubes from Ni-Co bimetallic catalysts
The effect of temperature variation on the growth of Carbon Nanotubes (CNTs) using Thermal Chemical Vapor Deposition (TCVD) is presented. Nickel and Cobalt (Ni-Co) thin films on Silicon (Si) substrates were used as catalysts in TCVD technique. Acetylene gas was used in CNTs growth process at the controlled temperature ranges from 850-1000 ̊ C. Catalysts and CNTs characterization was carried out ...
متن کاملInvestigating the Growth Process of Vertically Aligned Single-Walled Carbon Nanotubes Synthesized from Alcohol
We have performed a systematic investigation of the influence of growth parameters on the synthesis of vertically aligned single-walled carbon nanotubes (VA-SWNTs) by the alcohol catalytic chemical vapor deposition (ACCVD) method. The growth process of the VA-SWNTs was monitored using an in situ optical absorbance technique and the effects of CVD temperature and ethanol pressure on the initial ...
متن کاملLow-temperature growth of single-walled carbon nanotubes by water plasma chemical vapor deposition.
Preferential growth of pure single-walled carbon nanotubes (SWNTs) over multi-walled carbon nanotubes (MWNTs) was demonstrated at low temperature by water plasma chemical vapor deposition. Water plasma lowered the growth temperature down to 450 degrees C, and the grown nanotubes were single-walled without carbonaceous impurities and MWNTs. The preferential growth of pure SWNTs over MWNTs was pr...