Evaluation of adhesive bonding of ceramic tiles using active thermography

نویسنده

  • Luís Reis Santos
چکیده

Adhesion failure and/or detachment of ceramic tiling are common building defects. Bonding rupture of this type of coating presents a serious risk to people’s safety, in particular if it occurs on external façades. It may be avoided by earlier non-destructive inspections. This paper presents the results of an active thermography investigation in which adhesive bonding defects of ceramic coatings were examined. A set of non-destructive results was gathered based on a set of defects induced in the adhesive layer and an inappropriate adhesive technique or forced detachment between the ceramic tile and the bed layer.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Silane and bonding of Resins to Ceramic

Silane and bonding of Resins to Ceramic Dr. K. Seyyedan* - Dr. M. Kalalipoor** - Dr. M. Javan***Assistant Professor of Fixed Prosthodontics Dept., Faculty of Dentistry, Shaheed Beheshti University of Medical Sciences. **Resident of Fixed Prosthodontics Dept., Faculty of Dentistry, Shaheed Beheshti University of Medical Sciences. Background and Aim: When bonding between two different dental mate...

متن کامل

Large Area Active Brazing of Multi-tile Ceramic-Metal Structures

Lightweight ceramic-metal combinations are one option for advanced vehicle and other structural applications. These structures can require the fabrication of large area arrays of ceramic tiles on a metallic backing. However, the process of fabricating a combination of lightweight ceramics and metals is complicated by the need to bond these very dissimilar materials together. For severe applicat...

متن کامل

Natural radioactivity in ceramic tiles and associated radiological hazards

Background: The natural radioactivity levels in ceramic tiles produced in Turkey were determined and the related radiological hazards were assessed. Materials and Methods: The natural radioactivity levels (226Ra, 232Th and 40K) in the ceramic tiles were measured using high-purity germanium detector system (HPGe) and the related radiological hazards were assessed by radium equivalent activity (R...

متن کامل

Comparative evaluation of microleakage of composite restorations using fifth and seventh generations of adhesive systems

Introduction: Simultaneous etching of enamel and dentin using the novel generation of adhesive systems with contracted operational steps, has shown a good clinical efficacy. The aim of this study was to evaluate the microleakage of composite restorations using the V and VII generations of adhesive systems on primary teeth. Methods: This study was performed on 45 human intact extracted primar...

متن کامل

Defect detection in ceramic materials by quantitative infrared thermography

In this paper infrared (IR) measurements and dedicated signal processing algorithms were developed and applied for defect detection on green ceramic tiles. Tiles with defects having known dimension and position were realized and tested by acquiring either heating and cooling transients of the tile subjected to thermal pulse excitation. As rarely defects appear directly in the thermal map, post-...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2012