Glycerol is the main byproduct of biodiesel production and its increased production volume derives from the increasing demand for biofuels. The conversion of glycerol to hydrogen-rich mixtures presents an attractive route towards sustainable biodiesel production. Here we explored the use of Pt/Al(2)O(3)-based catalysts for the catalytic steam reforming of glycerol, evidencing the influence of La(2)O(3) and CeO(2) doping on the catalyst activity and selectivity. The addition of the latter metal oxides to a Pt/Al(2)O(3) catalyst is found to significantly improve the glycerol steam reforming, with high H(2) and CO(2) selectivities. A good catalytic stability is achieved for the Pt/La(2)O(3)/Al(2)O(3) system working at 350 degrees C, while the Pt/CeO(2)/Al(2)O(3) catalyst sharply deactivates after 20 h under similar conditions. Studies carried out on fresh and exhausted catalysts reveal that both systems maintain high surface areas and high Pt dispersions. Therefore, the observed catalyst deactivation can be attributed to coke deposition on the active sites throughout the catalytic process and only marginally to Pt nanoparticle sintering. This work suggests that an appropriate support composition is mandatory for preparing high-performance Pt-based catalysts for the sustainable conversion of glycerol into syngas.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Hydrogen Production by Steam Reforming of Ethanol on Rh-Pt Catalysts: Influence of CeO2, ZrO2, and La2O3 as Supports

CeO2-, ZrO2-, and La2O3-supported Rh-Pt catalysts were tested to assess their ability to catalyze the steam reforming of ethanol (SRE) for H2 production. SRE activity tests were performed using EtOH:H2O:N2 (molar ratio 1:3:51) at a gaseous space velocity of 70,600 h−1 between 400 and 700 °C at atmospheric pressure. The SRE stability of the catalysts was tested at 700 °C for 27 h time on stream ...

متن کامل

Steam reforming of propane over Ni-K/CeO2-Al2O3 catalyst in fluidized- and fixed-bed reactors under low steam to propane ratio

Fluidized bed was employed to investigate propane steam reforming over Ni-K/CeO2-Al2O3 catalyst. The catalyst was characterized by XRD, SEM, TG/DTA, and N2 adsorption-desorption tests. Effects of promoters, space velocity, temperature, and steam/propane (S/C) ratio on propane conversion, H2 yield, H2/CO ratio, and stability were studied and discussed. The experiments were carried out under cond...

متن کامل

Low temperature glycerol steam reforming on 1 bimetallic PtSn / C catalysts : on the effect of the Sn 2 content 3

Steam reforming of glycerol to produce syngas or H2-enriched streams is a 12 promising route that has caught the attention of many researchers around the world. This reaction 13 is typically carried out over metal-based catalysts supported on stable materials. Herein we report 14 a study on the effect of Sn on the catalytic properties of Pt/C in the aforementioned reaction. A 15 series of Pt-Sn...

متن کامل

Effects of Catalysts and Membranes on the Performance of Membrane Reactors in Steam Reforming of Ethanol at Moderate Temperature

Steam reforming of ethanol in the membrane reactor using the Pd77Ag23 membrane was evaluated in Ni/CeO2 and Co/CeO2 at atmospheric pressure. At 673 K, the H2 yield in the Pd77Ag23 membrane reactor over Co/CeO2 was found to be higher than that over Ni/CeO2, although the H2 yield over Ni/CeO2 exceeded that over Co/CeO2 at 773 K. This difference was owing to their reaction mechanism. At 773 K, the...

متن کامل

Hydrogen production by steam reforming of dimethyle ether over Cu/ZnO/Al2O3 and H-ZSM-5 catalysts: An experimental and modeling study

Hydrogen was produced by steam reforming of dimethyl ether (DME) using a physical mixture of commercial HZSM-5 zeolite (for DME hydrolyzing) and Cu/ZnO/Al2O3 (for methanol steam reforming) as a catalyst in a fixed bed reactor. The experiments were performed at atmospheric pressure and in a temperature range from 270 to 310 °C. The effects of feed temperature and gas hourly space velocity (GHSV)...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • ChemSusChem

دوره 3 5  شماره 

صفحات  -

تاریخ انتشار 2010