Hybrid xerogel films as novel coatings for antifouling and fouling release.
نویسندگان
چکیده
Hybrid sol-gel-derived xerogel films prepared from 45/55 (mol ratio) n-propyltrimethoxysilane (C3-TMOS)/tetramethylorthosilane (TMOS), 2/98 (mol ratio) bis[3-(trimethoxysilyl)propyl]-ethylenediamine (enTMOS)/tetraethylorthosilane (TEOS), 50/50 (mol ratio) n-octyltriethoxysilane (C8-TEOS)/TMOS, and 50/50 (mol ratio) 3,3,3-trifluoropropyltrimethoxysilane (TFP-TMOS)/TMOS were found to inhibit settlement of zoospores of the marine fouling alga Ulva (syn. Enteromorpha) relative to settlement on acid-washed glass and give greater release of settled zoospores relative to glass upon exposure to pressure from a water jet. The more hydrophobic 50/50 C8-TEOS/TMOS xerogel films had the lowest critical surface tension by comprehensive contact angle analysis and gave significantly greater release of 8-day Ulva sporeling biomass after exposure to turbulent flow generated by a flow channel than the other xerogel surfaces or glass. The 50/50 C8-TEOS/TMOS xerogel was also a fouling release surface for juveniles of the tropical barnacle Balanus amphitrite. X-ray photon electron data indicated that the alkylsilyl residues of the C3-TMOS-, C8-TEOS-, and TFP-TMOS-containing xerogels were located on the surface of the xerogel films (in a vacuum), which contributes to the film hydrophobicity. Similarly, the amine-containing silyl residues of the enTMOS/TEOS films were located at the surface of the xerogel films, which contributes to the more hydrophilic character and increased critical surface tension of these films.
منابع مشابه
Hydration and chain entanglement determines the optimum thickness of poly(HEMA-co-PEG₁₀MA) brushes for effective resistance to settlement and adhesion of marine fouling organisms.
Understanding how surface physicochemical properties influence the settlement and adhesion of marine fouling organisms is important for the development of effective and environmentally benign marine antifouling coatings. We demonstrate that the thickness of random poly(HEMA-co-PEG10MA) copolymer brushes affect antifouling behavior. Films of thicknesses ranging from 50 to 1000 Å were prepared vi...
متن کاملModern approaches to marine antifouling coatings
Marine structures such as platforms, jetties and ship hulls are subject to diverse and severe biofouling. Methods for inhibiting both organic and inorganic growth on wetted substrates are varied but most antifouling systems take the form of protective coatings. Biofouling can negatively affect the hydrodynamics of a hull by increasing the required propulsive power and the fuel consumption. This...
متن کاملAntifouling character of 'active' hybrid xerogel coatings with sequestered catalysts for the activation of hydrogen peroxide.
Halide-permeable xerogel films prepared from sols containing 50 mol% aminopropyltriethoxysilane (APTES)/50 mol% tetraethoxysilane (TEOS) or 10 mol% APTES/90 mol% TEOS and 0.015 M selenoxide or telluride catalyst in the sol gave reduced settlement of cypris larvae of the barnacle Balanus amphitrite and larvae of the tubeworm Hydroides elegans in the presence of artificial seawater (ASW) and hydr...
متن کاملSpontaneous multiscale phase separation within fluorinated xerogel coatings for fouling-release surfaces.
Four-component xerogel films consisting of 1 mole-% n-octadecyltrimethoxysilane (C18) and 50 mole-% tetraethoxysilane (TEOS) in combination with 1-24 mole-% tridecafluoro-1,1,2,2-tetrahydrooctyltriethoxysilane (TDF) and 25-48 mole-% n-octyltriethoxysilane (C8) and a 1:49:50 mole-% C18/TDF/TEOS were prepared. Settlement of barnacle cyprids and removal of juvenile barnacles, settlement of zoospor...
متن کاملTemporal and Spatial Variations in Macrofouling of Silicone Fouling-Release Coatings
Nontoxic, low surface free energy silicone coatings having reduced biofouling adhesion strength have been developed as an alternative to antifouling paints. Silicone coatings permit macrofouling to adhere; however, fouling can be removed easily by water pressure or light scrubbing. One of the current methods used to evaluate the performance of non-toxic silicone foulingrelease coatings relies h...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Biofouling
دوره 21 1 شماره
صفحات -
تاریخ انتشار 2005