Fabrication of Poly(p-oxybenzoyl) Nanowhisker
نویسندگان
چکیده
Fabrication of poly(p-oxybenzoyl) (POB) nanowhiskers was examined by using reaction-induced crystallization of oligomers during the polymerization of p-acetoxybenzoic acid in liquid paraffin. Width of the POB whiskers was susceptible to polymerization temperature and it was efficiently controlled by a change in temperature during the polymerization. Increase in polymerization temperature just after nucleation (Han) reduced the degree of super saturation of oligomers ( ) resulting in the depression of the width increase by the crystallization of oligomers on side surface of the whiskers. Temperature drop just before nucleation (Cbn) enhanced the value of resulting in the generation of much more nuclei having the smaller width. On the basis of these results, the combination of these two methods Han and Cbn afforded the whiskers having the smallest width, and the POB nanowhiskers were prepared of which the width and the length were 190 nm and 18.6 mm, respectively. [DOI 10.1295/polymj.37.906]
منابع مشابه
Fabrication of Free-Standing Tungsten-Nanowhiskers on SiO2 Substrates with Electron-Beam Induced Deposition
Free-standing tungsten-nanowhiskers about 3 nm in thickness were fabricated on SiO2 substrates with electron-beam induced deposition in a transmission electron microscope operated at 400 kV at room temperature. The growth process of the nanowhisker was observed in-situ and analyzed. The nanowhisker was characterized with high-resolution transmission electron microscopy. Nucleus-deposits smaller...
متن کاملFabrication of Ordered Mullite Nanowhisker Array with Surface Enhanced Raman Scattering Effect
Mullite nanowhiskers are prepared by a facile technique at low temperature using mica and AlF3 as raw material. Mica acts as reactant as well as substrate. By controlling the reaction temperature and holding time, the mullite nanowhisker array with uniform morphology is obtained. The nanowhisker array possesses Al-rich single crystalline with an average of 80 nm in diameter and 20 μm in length....
متن کاملEffect of SiC Nanowhisker on the Microstructure and Mechanical Properties of WC-Ni Cemented Carbide Prepared by Spark Plasma Sintering
Ultrafine tungsten carbide-nickel (WC-Ni) cemented carbides with varied fractions of silicon carbide (SiC) nanowhisker (0-3.75 wt.%) were fabricated by spark plasma sintering at 1350°C under a uniaxial pressure of 50 MPa with the assistance of vanadium carbide (VC) and tantalum carbide (TaC) as WC grain growth inhibitors. The effects of SiC nanowhisker on the microstructure and mechanical prope...
متن کاملEfficiency improvement of silicon solar cells enabled by ZnO nanowhisker array coating
An efficient antireflection coating is critical for the improvement of silicon solar cell performance via increased light coupling. Here, we have grown well-aligned ZnO nanowhisker (NW) arrays on Czochralski silicon solar cells by a seeding-growth two-step process. It is found that the ZnO NWs have a great effect on the macroscopic antireflection effect and, therefore, improves the solar cell p...
متن کاملFabrication of Polyvinyl Alcohol/Kefiran Nanofibers Membrane Using Electrospinning
The Poly (vinyl alcohol)/Kefirane nanofiber membrane was successfully fabricated for the firsttime using electrospinning of the polyvinyl alcohol (PVA) and Kefirane blend solution. Scanningelectron microscope (SEM), attenuated total reflectance Fourier transform infrared (ATRFT-IR), and differential scanning calorimetry (DSC) were used to characterize the electrospunPoly (vinyl alcohol)/Kefiran...
متن کامل