چکیده

The non-destructive testing of austenitic welds using ultrasound plays an important role in the assessment of the structural integrity of safety critical structures. The internal microstructure of these welds is highly scattering and can lead to the obscuration of defects when investigated by traditional imaging algorithms. This paper proposes an alternative objective method for the detection of flaws embedded in austenitic welds based on the singular value decomposition of the time-frequency domain response matrices. The distribution of the singular values is examined in the cases where a flaw exists and where there is no flaw present. A lower threshold on the singular values, specific to austenitic welds, is derived which, when exceeded, indicates the presence of a flaw. The detection criterion is successfully implemented on both synthetic and experimental data. The datasets arising from welds containing a flaw are further interrogated using the decomposition of the time-reversal operator (DORT) method and the total focusing method (TFM), and it is shown that images constructed via the DORT algorithm typically exhibit a higher signal-to-noise ratio than those constructed by the TFM algorithm.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Interface and Heat-affected Zone Features of Dissimilar Welds between AISI 310 Austenitic Stainless Steel and Inconel 657

The aim of this paper is to characterize welding of AISI 310 austenitic stainless steel to Inconel 657 for use in oil-refining industries. The welds were produced using four types of filler materials; nickel-based alloys designated as Inconel 82, A, 617, and 310 SS. The interfaces and heat-affected zones were characterized by optical and scanning electron microscopy. Interfaces on the two sides...

متن کامل

Structure-property Interaction in Flux Assisted Tungsten Inert Gas Welding of Austenitic Stainless Steel

Austenitic stainless steel SS304 grade was welded with active Tungsten Inert Gas (TIG) welding process by applying a flux paste made of SiO2 powder and acetone. SiO2 flux application improves the weld bead depth with a simultaneous reduction in weld bead width. The improvement in penetration results from arc constriction and reversal of Marangoni convection. Experimental studies revealed that t...

متن کامل

A Comparative Evaluation of Welding Consumables for Dissimilar Welds between 310 Austenitic Stainless Steel and Inconel 657

The current work was carried out to characterize welding of AISI 310 austenitic stainless steel to Inconel 657 nickel-chromium superalloy. The welds were produced using four types of filler materials; the nickel-based corresponding to Inconel 82, Inconel A, Inconel 617 and austenitic stainless steels 310. Of the two joints involved, this paper describes the choice of welding consumables for the...

متن کامل

The Evaluation of Corrosion Behavior of AISI 347 Stainless Steel to ASTM A335 Low Alloy Steel Dissimilar Welds

In the present study, the corrosion behavior of AISI 347 austenitic stainless steel to ASTM A335 low alloy steel dissimilar joint was investigated. For this purpose, two filler metals, ER309L and ERNiCr-3, were selected to be used during the gas tungsten arc welding process. To investigate the corrosion behavior of the joints after welding, the specimens were tested in 3.5% sodium chloride solu...

متن کامل

The Weldability Evaluation of Dissimilar Welds of AISI 347 Stainless Steel to ASTM A335 Low Alloy Steel by Gastungesten Arc Welding

In the present study, the Weldability and microstructure of dissimilar welds of AISI 347austenitic stainless steel to ASTM A335 low alloy steel was investigated. For this purpose, gas tungsten arc welding process and two filler metals including ERNICr-3 and ER309L were used. After welding, the microstructure of the different zones of each joint, including weld metals, heat affected zone (HAZ) 1...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 472  شماره 

صفحات  -

تاریخ انتشار 2016