Fretting wear in aluminium alloy AA5754 joined by self-pierce riveting (SPR), a relatively new fastening technique increasingly used in vehicle structures, has been investigated in this paper. Surface damages have been induced when a joint experienced a sinusoidal cyclic tension-tension load. Various degradation zones have been characterised in the contact surfaces between the aluminium sheets, as well as the rivet and the locked sheet. Subsequent examination of the fretting scars at the contact surfaces and through the cross-section has been carried out using optical and scanning electron microscopies. The fretting patterns in the self-piercing riveted joints have been identified. It was noted that fretting wear was initially patchy and layers of compacted debris were created as fretting continued. An Energy Dispersive X-ray (EDX) analysis of the fretting debris from the interface between the rivet and the aluminium sheet revealed the presence of Al, Fe, Si, C and O so that it is suggested that intimate mixing of debris from the aluminium alloy and the steel rivet had occurred. The effects of testing conditions such as the load magnitude and the number of loading cycles on the fretting wear patterns were also studied. Metallographic examination has shown that these fretting zones are critical with respect to fretting crack nucleation. The test results have shown that joint fracture initiates at these critical zones.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Mechanical Behaviour and Corrosion of Interstitial-free Steel Aluminium Alloy Self-piercing Riveted Joints

.......................................................................................i-ii ACKNOWLEDGEMENTS...................................................................iii-iv CONTENTS......................................................................................v-vii LIST OF FIGURES...........................................................................viii-xiii LIST OF TABLES....

متن کامل

Fretting Behavior of SPR Joining Dissimilar Sheets of Titanium and Copper Alloys

The fretting performance of self-piercing riveting joining dissimilar sheets in TA1 titanium alloy and H62 copper alloy was studied in this paper. Load-controlled cyclic fatigue tests were carried out using a sine waveform and in tension-tension mode. Scanning electron microscopy and energy-dispersive X-ray techniques were employed to analyze the fretting failure mechanisms of the joints. The e...

متن کامل

Surface morphology in engineering applications: Influence of roughness on sliding and wear in dry fretting

Influence of initial surface roughness on friction and wear processes under fretting conditions was investigated experimentally. Rough surfaces (Ra=0.15-2.52 μm) were prepared on two materials: carbon alloy (AISI 1034) and titanium alloy (Ti-6Al-4V). Strong influence of initial surface roughness on friction and wear processes is reported for both tested materials. Lower coefficient of friction ...

متن کامل

Crack Behavior of the Aluminum Alloy 2024 Under Fretting Conditions

The initial stage of fretting fatigue crack growth is significantly influenced by tangential force induced by fretting action along the contact surface where a mixed-mode crack growth is involved. Fretting crack behavior of aluminum alloy 2024 was studied, taking into account the problem of contact asperities. Finite element was used for the determination of the stress field near the contact su...

متن کامل

Effects of Plasma ZrN Metallurgy and Shot Peening Duplex Treatment on Fretting Wear and Fretting Fatigue Behavior of Ti6Al4V Alloy

A metallurgical zirconium nitride (ZrN) layer was fabricated using glow metallurgy using nitriding with zirconiuming prior treatment of the Ti6Al4V alloy. The microstructure, composition and microhardness of the corresponding layer were studied. The influence of this treatment on fretting wear (FW) and fretting fatigue (FF) behavior of the Ti6Al4V alloy was studied. The composite layer consiste...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2008