Uniform and accelerated degradation of pure iron patterned by Pt disc arrays
نویسندگان
چکیده
Pure iron has been confirmed as a promising biodegradable metal. However, the degradation rate of pure iron should be accelerated to meet the clinical requirements. In this work, two different designs of platinum disc arrays, including sizes of Φ20 μm × S5 μm and Φ4 μm × S4 μm, have been coated on the surface of pure iron. Corrosion tests showed the platinum discs formed plenty of galvanic cells with the iron matrix which significantly accelerated the degradation of pure iron. Simultaneously, due to the designability of the shape, size as well as distribution of Pt discs, the degradation rate as well as degradation uniformity of pure iron can be effectively controlled by coating with platinum discs. The cytotoxicity test results unveiled that Pt discs patterned pure iron exhibited almost no toxicity to human umbilical vein endothelial cells, but a significant inhibition on proliferation of vascular smooth muscle cells. In addition, the hemolysis rate of Pt discs patterned pure iron was lower than 1%. Moreover, Pt discs also effectively reduced the number of adhered platelets. All these results indicated that Pt discs patterning is an effective way to accelerate degradation and improve biocompatibility of pure iron.
منابع مشابه
Design of Highly Uniform Platinum and Palladium Nanoparticle Decoration on TiO2 Nanotube Arrays: An Efficient Anode to the Electro-Oxidation of Alcohols
We explore electro-catalytic properties of a system consisting of platinum and palladium nanoparticles dispersed over a nanotubular self-organized TiO2 matrix. These electrodes prepared by electroess and microemulsion of palladium and palladium nanoparticles on to TiO2 nanotubes, respectively. Titanium oxide nanotubes were fabricated by anodizing titanium foil in ethylene glycol (EG) fluoride-c...
متن کاملPhotocatalytic degradation of E. coli bacteria using TiO2/SiO2 nanoparticles with photodeposited platinum
In this work, TiO2 /SiO2 (pure anatase), and TiO2 /SiO2 (anatase/rutile) nano-photocatalysts are prepared by using sol-gel method and control of acidity. The particles size is calculated using Scheerer, s equation and is estimated to be around 7-15 nm. In order to improve the photocatalytic activity of TiO2 /SiO2 ,1% (wt) platinum particles are loaded on both catalysts using photoreductive meth...
متن کاملAccelerating degradation rate of pure iron by zinc ion implantation
Pure iron has been considered as a promising candidate for biodegradable implant applications. However, a faster degradation rate of pure iron is needed to meet the clinical requirement. In this work, metal vapor vacuum arc technology was adopted to implant zinc ions into the surface of pure iron. Results showed that the implantation depth of zinc ions was about 60 nm. The degradation rate of p...
متن کاملMonodisperse pattern nanoalloying for synergistic intermetallic catalysis.
Nanoscale alloys attract enormous research attentions in catalysis, magnetics, plasmonics and so on. Along with multicomponent synergy, quantum confinement and extreme large surface area of nanoalloys offer novel material properties, precisely and broadly tunable with chemical composition and nanoscale dimension. Despite substantial progress of nanoalloy synthesis, the randomized positional arr...
متن کاملMagnetic reversal of ion beam patterned Co/Pt multilayers
The characteristics of the reversal processes of magnetic arrays fabricated by ion-irradiation of Co/Pt multilayers with perpendicular magnetic anisotropy are reported. Magnetic patterns with periodicities from 1 lm to 100 nm were patterned. A correlation between the pattern size, magnetic reversal and grain size is presented. 2003 Acta Materialia Inc. Published by Elsevier Science Ltd. All rig...
متن کامل