Morphologies of tungsten nanotendrils grown under helium exposure
نویسندگان
چکیده
Nanotendril "fuzz" will grow under He bombardment under tokamak-relevant conditions on tungsten plasma-facing materials in a magnetic fusion energy device. We have grown tungsten nanotendrils at low (50 eV) and high (12 keV) He bombardment energy, in the range 900-1000 °C, and characterized them using electron microscopy. Low energy tendrils are finer (~22 nm diameter) than high-energy tendrils (~176 nm diameter), and low-energy tendrils have a smoother surface than high-energy tendrils. Cavities were omnipresent and typically ~5-10 nm in size. Oxygen was present at tendril surfaces, but tendrils were all BCC tungsten metal. Electron diffraction measured tendril growth axes and grain boundary angle/axis pairs; no preferential growth axes or angle/axis pairs were observed, and low-energy fuzz grain boundaries tended to be high angle; high energy tendril grain boundaries were not observed. We speculate that the strong tendency to high-angle grain boundaries in the low-energy tendrils implies that as the tendrils twist or bend, strain must accumulate until nucleation of a grain boundary is favorable compared to further lattice rotation. The high-energy tendrils consisted of very large (>100 nm) grains compared to the tendril size, so the nature of the high energy irradiation must enable faster growth with less lattice rotation.
منابع مشابه
Damage studies on irradiated tungsten by helium and argon ions in a plasma focus device
Damage of tungsten due to helium and argon ions of a PF device was studied. Tungsten samples were irradiated by 20 shots of the plasma focus device with argon and helium as working gases, separately. The tungsten surface was analyzed by SEM, before and after irradiation. SEM revealed dense blisters with diameters of a few hundred nanometers, on the samples which were irradiated by helium ions, ...
متن کاملDynamic measurement of the helium concentration of evolving tungsten nanostructures using Elastic Recoil Detection during plasma exposure
Helium (He) concentration depth profiles of evolving tungsten (W) nanostructures have been measured for the first time using in situ Elastic Recoil Detection (ERD) throughout plasma irradiation. Exposures resulting in fuzzy and non-fuzzy surfaces were analyzed in order to illuminate the role of He during the development of these surface morphologies. ERD was performed on samples with surface te...
متن کاملThe impact of doping rates on the morphologies of silver and gold nanowires grown in helium nanodroplets.
Silver and gold nanowires are grown within superfluid helium nanodroplets and investigated by high resolution electron microscopy after surface deposition. The wire morphologies depend on the rate of metal atom doping in the pickup sequence. While high doping rates result in a polycrystalline face-centered cubic nanowire structure, at lower doping rates the initial fivefold-symmetry seems to be...
متن کاملHelium bubble formation in ultrafine and nanocrystalline tungsten under different extreme conditions
We have investigated the effects of helium ion irradiation energy and sample temperature on the performance of grain boundaries as helium sinks in ultrafine grained and nanocrystalline tungsten. Irradiations were performed at displacement and non-displacement energies and at temperatures above and below that required for vacancy migration. Microstructural investigations were performed using Tra...
متن کاملDirect time-resolved observation of tungsten nanostructured growth due to helium plasma exposure
Determination of the mechanisms underlying the growth of tungsten fuzz is an important step towards mitigation of fuzz formation. Nanostructured tungsten was produced on resistively heated tungsten wires in a helicon plasma source (maximum flux of 2.5× 1021 m−2 s−1). Asymmetry in the setup allows for investigation of temperature and flux effects in a single sample. An effort at elucidating the ...
متن کامل