Comparative Reliability Studies and Analysis of Au, Pd-Coated Cu and Pd-Doped Cu Wire in Microelectronics Packaging
نویسندگان
چکیده
This paper compares and discusses the wearout reliability and analysis of Gold (Au), Palladium (Pd) coated Cu and Pd-doped Cu wires used in fineline Ball Grid Array (BGA) package. Intermetallic compound (IMC) thickness measurement has been carried out to estimate the coefficient of diffusion (Do) under various aging conditions of different bonding wires. Wire pull and ball bond shear strengths have been analyzed and we found smaller variation in Pd-doped Cu wire compared to Au and Pd-doped Cu wire. Au bonds were identified to have faster IMC formation, compared to slower IMC growth of Cu. The obtained weibull slope, β of three bonding wires are greater than 1.0 and belong to wearout reliability data point. Pd-doped Cu wire exhibits larger time-to-failure and cycles-to-failure in both wearout reliability tests in Highly Accelerated Temperature and Humidity (HAST) and Temperature Cycling (TC) tests. This proves Pd-doped Cu wire has a greater potential and higher reliability margin compared to Au and Pd-coated Cu wires.
منابع مشابه
More uniform Pd distribution in free-air balls of Pd-coated Cu bonding wire using movable flame-off electrode
The currently high price of gold wire has led to the development of bonding wire made from palladium-coated-copper as a lower cost alternative. Increasing the uniformity of the Pd distribution in free-air balls, formed by melting the wire end with an electric spark, is of interest as it can influence the uniformity of process and reliability. To study this Pd distribution, free-air balls are ma...
متن کاملEffects of Current Stressing on the Grain Structure and Mechanical Properties of Ag-Alloy Bonding Wires with Various Pd and Au Contents
Ag-alloy bonding wires containing various Pd and Au elements and traditional 4 N Au and Pd-coated 4 N Cu bonding wires were stressed with a current density of 1.23 ˆ 105 A/cm2 in air. The amounts of annealing twins in the Ag-alloy wires were much higher than those in Au and Pd-coated Cu wires. The percentages of twinned grains in these Ag-alloy wires increased obviously with current stressing. ...
متن کاملEffect of Pd Surface Roughness on the Bonding Process and High Temperature Reliability of Au Ball Bonds
A 0.3-lm-thick electrolytic Pd layer was plated on 1 lm of electroless Ni on 1 mm-thick polished and roughened Cu substrates with roughness values (Ra) of 0.08 lm and 0.5 lm, respectively. The rough substrates were produced with sand-blasting. Au wire bonding on the Ni/Pd surface was optimized, and the electrical reliability was investigated under a high temperature storage test (HTST) during 8...
متن کاملRole of impact ultrasound on bond strength and Al pad splash in Cu wire bonding
Cu wire is replacing Au wire in the microelectronic industry due to its lower cost. However, during Cu ball bonding one of the main challenges is the increased stress that can damage the pad and underpad layers. Past work showed that using ultrasound superimposed together with impact force (pre-ultrasound) results not only in a softer bonded ball, but also in a flatter ball/pad interface. In th...
متن کاملRole of process parameters on bondability and pad damage indicators in copper ball bonding
Cu wire bonding is one of the hottest trends in electronic packaging due to the cost and performance advantages of Cu wire over Au wire. However, there are many challenges to Cu wire bonding, one of which is the increased stress transmitted to the bond pad during bonding. This high stress is not desirable as it leads to pad damage or cratering in the Si under the pad. Another issue is pad splas...
متن کامل