Evaluation of ionic degradation and slot corrosion of metallic brackets by the action of different dentifrices.
نویسندگان
چکیده
OBJECTIVE To evaluate the in vitro ionic degradation and slot base corrosion of metallic brackets subjected to brushing with dentifrices, through analysis of chemical composition by Energy Dispersive Spectroscopy (EDS) and qualitative analysis by Scanning Electron Microscopy (SEM). METHODS Thirty eight brackets were selected and randomly divided into four experimental groups (n = 7). Two groups (n = 5) worked as positive and negative controls. Simulated orthodontic braces were assembled using 0.019 x 0.025-in stainless steel wires and elastomeric rings. The groups were divided according to surface treatment: G1 (Máxima Proteção Anticáries®); G2 (Total 12®); G3 (Sensitive®); G4 (Branqueador®); Positive control (artificial saliva) and Negative control (no treatment). Twenty eight brushing cycles were performed and evaluations were made before (T0) and after (T1) experiment. RESULTS The Wilcoxon test showed no difference in ionic concentrations of titanium (Ti), chromium (Cr), iron (Fe) and nickel (Ni) between groups. G2 presented significant reduction (p < 0.05) in the concentration of aluminium ion (Al). Groups G3 and G4 presented significant increase (p < 0.05) in the concentration of aluminium ion. The SEM analysis showed increased characteristics indicative of corrosion on groups G2, G3 and G4. CONCLUSION The EDS analysis revealed that control groups and G1 did not suffer alterations on the chemical composition. G2 presented degradation in the amount of Al ion. G3 and G4 suffered increase in the concentration of Al. The immersion in artificial saliva and the dentifrice Máxima Proteção Anticáries® did not alter the surface polishing. The dentifrices Total 12®, Sensitive® and Branqueador® altered the surface polishing.
منابع مشابه
Galvanic Corrosion among Different Combination of Orthodontic Archwires and Stainless Steel Brackets
Introduction: The aim of this study was to assess the galvanic behavior of different bracket and archwire combinations that are commonly used in orthodontic treatments. Methods: Three types of orthodontic archwires with a diameter of 0.016×0.022 inch and 80 standard edgewise maxillary central incisor brackets were selected. Three groups consisted of different wire-bracket couples and one group ...
متن کاملGalvanic Corrosion of Orthodontic Brackets and Wires in Acidic Artificial Saliva: Part II
Objective: Orthodontic wires should have high resistance against corrosion in the oral environment. Since the effect of pH on corrosion has been well recognized, this study sought to assess and compare the electrochemical corrosion of orthodontic brackets and wires of different brands in acidic artificial saliva. Methods: This in vitro experimental study was conducted on 24 mandibular centr...
متن کاملGalvanic Corrosion and Ion Release from Different Orthodontic Brackets and Wires in Acidic Artificial Saliva: Part I
Objective: Corrosion resistance is among the most important properties of metal alloys used in the oral cavity. Consumption of acidic foods reduces the salivary pH and intensifies the corrosion of brackets and orthodontic wires. This study aimed to compare electro galvanic corrosion of different orthodontic brackets and wires and determine the amount of ions released into acidic artifici...
متن کاملShear Bond Strength of Metallic and Ceramic Brackets Bonded with Two-step and Three-step Light Cure Adhesives
Background and purpose: The bonding process is highly important in orthodontic treatment for its fast speed. The purpose of this study was to compare the shear bond strength of ceramic and metallic brackets between three stage (transbondTM XT) and two stage (GC ortho connectTM) light cure composites. Materials and methods: In this experimental study, 80 maxillary and mandibular first and sec...
متن کاملComparison of shear bond strength of the stainless steel metallic brackets bonded by three bonding systems
Introduction: In orthodontic treatment, it is essential to establish a satisfactory bond between enamel and bracket. After the self-etch primers (SEPs) were introduced for the facilitation of bracket bonding in comparison to the conventional etch-and-bond system, multiple studies have been carried out on their shear bond strengths which have yielded different results. This study was aimed at co...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Dental press journal of orthodontics
دوره 18 1 شماره
صفحات -
تاریخ انتشار 2013