Effect of interfacial variables on metal-porcelain bonding.

نویسندگان

  • W C Wagner
  • K Asgar
  • W C Bigelow
  • R A Flinn
چکیده

While ceramic-to-metal bonding has been used in many applications, the actual chemical and physical factors leading to optimum bond strength are not well understood. In this work, several variables affecting the bonding between dental porcelain and a palladium alloy (85% Pd, 10% Cu, and 5% Ga) were investigated: 1) precoating the metal by sputtering various oxides before porcelaining; 2) peroxidation of the metal base before porcelaining; 3) porcelaining under reducing atmosphere; and 4) surface roughening at controlled levels before porcelaining. Using a modification of the push doughnut shear bond strength test to measure bond strength the following results were obtained. 1) Compared with standard "control" samples, the aluminum oxide precoated specimens showed a bond strength improvement of 46%, while the copper, manganese, and tin oxide precoatings exhibited smaller effects. 2) Preoxidation of the metal base led to pronounced bond strengthening (152%) by surface roughening as well as oxide formation. 3) Porcelaining under a reducing atmosphere severely reduced bond strength (88% lower than the controls) indicating the role of oxidation during the standard firing cycle. 4) Mechanical roughening of the surface by controlled amounts gave pronounced improvements with greater notch depth. Coarse roughening produced the highest bond strength improvements (486%).

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Comparison of the Effect of Three methods of Porcelain Surface Treatment on Shear Bond Strength of Composite to Porcelain

Background and Aim: Several methods are available for intraoral repair of chipped porcelain restorations by composite resin. Also, there is still controversy regarding the best method of porcelain repair in terms of bond strength and cost effectiveness. This study aimed to compare three methods of porcelain surface treatment on shear bond strength (SBS) of composite to porcelain. Materials a...

متن کامل

بررسی اثر پخت مکرر پرسلن بر مقاومت باند در دو نوع آلیاژ بیس متال (مینالوکس و وراباند 2)

The formation of oxides on the surface of the metal are proven to contribute to the formation of strong bonding. However, The base metal alloys are expected to exhibit more oxidation than high gold alloys, increase in oxide layer thickness due to repeated firing in them can reduce the bond strength. The aim of this study was to compare the effect of repeated porcelain firing on the bond strengt...

متن کامل

Effect of metal conditioner on bonding of porcelain to cobalt-chromium alloy

PURPOSE The purpose of this study was to evaluate the efficacy of two different metal conditioners for non-precious metal alloys for the bonding of porcelain to a cobalt-chromium (Co-Cr) alloy. MATERIALS AND METHODS Disk-shaped specimens (2.5×10.0 mm) were cast with Co-Cr alloy and used as adherend materials. The bonding surfaces were polished with a 600-grid silicon carbide paper and airborn...

متن کامل

The Application of a Novel Ceramic Liner Improves Bonding between Zirconia and Veneering Porcelain

The adhesion of porcelain to zirconia is a key factor in the success of bilayered restorations. In this study, the efficacy of a novel experimental liner (EL) containing zirconia for improved bonding between zirconia and veneering porcelain was tested. Four ELs containing various concentrations (0, 3.0, 6.0, and 9.0 wt %) of zirconia were prepared. Testing determined the most effective EL (EL3 ...

متن کامل

Effects of metal surface grinding at the porcelain try-in stage of fixed dental prostheses

PURPOSE This study was to evaluate the effect of grinding of the inner metal surface during the porcelain try-in stage on metal-porcelain bonding considering the maximum temperature and the vibration of samples. MATERIALS AND METHODS Ninety-one square prism-shaped (1 × 1 × 1.5 mm) nickel-chrome cast frameworks 0.3 mm thick were prepared. Porcelain was applied on two opposite outer axial surfa...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of biomedical materials research

دوره 27 4  شماره 

صفحات  -

تاریخ انتشار 1993