Biosafety of the Novel Vancomycin-loaded Bone-like Hydroxyapatite/Poly-amino Acid Bony Scaffold
نویسندگان
چکیده
BACKGROUND Recently, local sustained-release antibiotics systems have been developed because they can increase local foci of concentrated antibiotics without increasing the plasma concentration, and thereby effectively decrease any systemic toxicity and side effects. A vancomycin-loaded bone-like hydroxyapatite/poly-amino acid (V-BHA/PAA) bony scaffold was successfully fabricated with vancomycin-loaded poly lactic-co-glycolic acid microspheres and BHA/PAA, which was demonstrated to exhibit both porosity and perfect biodegradability. The aim of this study was to systematically evaluate the biosafety of this novel scaffold by conducting toxicity tests in vitro and in vivo. METHODS According to the ISO rules for medical implant biosafety, for in vitro tests, the scaffold was incubated with L929 fibroblasts or rabbit noncoagulant blood, with simultaneous creation of positive control and negative control groups. The growth condition of L929 cells and hemolytic ratio were respectively evaluated after various incubation periods. For in vivo tests, a chronic osteomyelitis model involving the right proximal tibia of New Zealand white rabbits was established. After bacterial identification, the drug-loaded scaffold, drug-unloaded BHA/PAA, and poly (methyl methacrylate) were implanted, and a blank control group was also set up. Subsequently, the in vivo blood drug concentrations were measured, and the kidney and liver functions were evaluated. RESULTS In the in vitro tests, the cytotoxicity grades of V-BHA/PAA and BHA/PAA-based on the relative growth rate were all below 1. The hemolysis ratios of V-BHA/PAA and BHA/PAA were 2.27% and 1.42%, respectively, both below 5%. In the in vivo tests, the blood concentration of vancomycin after implantation of V-BHA/PAA was measured at far below its toxic concentration (60 mg/L), and the function and histomorphology of the liver and kidney were all normal. CONCLUSION According to ISO standards, the V-BHA/PAA scaffold is considered to have sufficient safety for clinical utilization.
منابع مشابه
In vitro and in vivo drug release and antibacterial properties of the novel vancomycin-loaded bone-like hydroxyapatite/poly amino acid scaffold
Antibiotic-loaded carriers were developed to fill cavities and locally deliver antibiotics following implantation. However, the most commonly used antibiotic carrier, polymethyl methacrylate (PMMA), has many disadvantages including that it does not promote bone regeneration or conduction. Vancomycin-loaded bone-like hydroxyapatite/poly amino acid (V-BHA/PAA) was successfully fabricated by a hom...
متن کاملComparison of Proliferation and Osteoblast Differentiation of Marrow-Derived Mesenchymal Stem Cells on Nano- and Micro-Hydroxyapatite Contained Composite Scaffolds
Bones constructed by tissue engineering are being considered as valuable materials to be used for regeneration of large defects in natural bone. In an attempt to prepare a new bone construct, in this study, proliferation and bone differentiation of marrow-derived mesenchymal stem cells (MSCs) on our recently developed composite scaffolds of nano-, micro-hydroxyapatite/ poly(l-lactic acid) were ...
متن کاملReconstructionof Human Mandibular Continuity Defects with Allogenic Scaffold and Autologousmarrow Mesenchymal Stem Cells
Background Mandibular continuity defects occur after tumor resection, maxillofacial injury, or osteomyelitis. Despite the current availability of a plethora of treatment modalities, bone substitutes, and various clinical adjuncts, an exact reconstructive recapitulation of large bony defects continues to be beyond reach. In this clinical pilot study, we report a novel method for reconstruction ...
متن کاملIn vitro and In vivo Investigation of poly(lactic acid)/hydroxyapatite nanoparticle scaffold containing nandrolone decanoate for the regeneration of critical-sized bone defects
Objective(s): Bone tissue engineering is aimed at the fabrication of bone graft to ameliorate bone defects without using autografts or allografts. Materials and Methods: In the present study, the coprecipitation method was used to prepare hydroxyapatite (HA) nanoparticles containing nandrolone. To do so, 12.5, 25, and 50 mg of nandrolone were loaded into poly(lactic acid) (PLA)/nano-HA, a...
متن کاملTreating Proximal Tibial Growth Plate Injuries Using Poly(Lactic-co-Glycolic Acid) Scaffolds
Growth plate fractures account for nearly 18.5% of fractures in children. Depending on the type and severity of the injury, inhibited bone growth or angular deformity caused by bone forming in place of the growth plate can occur. The current treatment involves removal of the bony bar and replacing it with a filler substance, such as a free fat graft. Unfortunately, reformation of the bony bar f...