Europium-doped yttrium silicate nanophosphors prepared by flame synthesis
نویسندگان
چکیده
Europium-doped yttrium silicate (Y2SiO5:Eu ) nanophosphors were successfully synthesized by flame spray pyrolysis method. The effect of silicon concentration on the crystal structure and morphology of the Y2SiO5:Eu 3+ phosphors were investigated. Asprepared phosphor consists of spherical nanoparticles with filled morphology, high crystallinity, narrow size distribution, and intense photoluminescence. The crystal structure and photoluminescence intensity of Y2SiO5:Eu 3+ nanophosphors are strongly affected by the ratio of silicon to yttrium in the precursor solution, and the maximum photoluminescence intensity is obtained from particles prepared from the silicon to yttrium ratio of 1.25. A concentration quenching limit is observed at 30 mol% Eu of yttrium. The photoluminescence intensity also increases with the increase of the concentration of precursor solution. This work demonstrates the advantages of flame spray pyrolysis method for the preparation of multi-component nanophosphor, which can be found potential application in lamp and display industries. # 2006 Elsevier Ltd. All rights reserved.
منابع مشابه
Continuous Liquid Phase Synthesis of Europium and Bismuth Co-Doped Yttrium Vanadate Nanophosphor Using Microwave Heating
A continuous flow reactor equipped with a low-loss flow channel and a microwave cavity was developed for synthesizing nanophosphors. A continuous solution synthesis of YVO4:Eu,Bi nanophosphor was succeeded through the rapid hydrothermal method using this equipment. Internal quantum efficiency of YVO4:Eu,Bi nanophosphor obtained by 20 minutes microwave heating is about 30% at 320 nm as high as t...
متن کاملSynthesis and functionalization of monodisperse near-ultraviolet and visible excitable multifunctional Eu(3+), Bi(3+):REVO4 nanophosphors for bioimaging and biosensing applications.
Near-ultraviolet and visible excitable Eu- and Bi-doped NPs based on rare earth vanadates (REVO4, RE = Y, Gd) have been synthesized by a facile route from appropriate RE precursors, europium and bismuth nitrate, and sodium orthovanadate, by homogeneous precipitation in an ethylene glycol/water mixture at 120 °C. The NPs can be functionalized either by a one-pot synthesis with polyacrylic acid (...
متن کاملReddish - orange Ca 3 x Al 2 O 6 : x Eu 3 þ nanophosphors : Fast synthesis and photophysical properties
This paper focuses on the synthesis and the photoluminescent properties of Ca3 xAl2O6:xEu 3þ (0rxr0.1) nanophosphors prepared by microwave-assisted combustion method without any further heat treatment. X-ray diffraction, scanning electron microscopy and photoluminescence spectroscopy were used to characterize the produced samples. Nanosized particles smaller than 120 nmwere obtained as confirme...
متن کاملSurface modified Eu:GdVO4 nanocrystals for optical and MRI imaging.
A facile solvothermal route has been developed for the preparation of europium doped gadolinium orthovanadate nanoparticles (~70 nm) with tetragonal structure, based on a homogenous precipitation reaction at 120 °C from rare earth precursors (yttrium nitrate and europium nitrate) and sodium orthovanadate solutions using an ethylene glycol-water mixture as the solvent. The effects of the doping ...
متن کاملFlame synthesis of Y2O3:Eu nanophosphors using ethanol as precursor solvents
Y2O3:Eu nanophosphors were prepared by flame synthesis using ethanol or water as precursor solutions. The effects of precursor solvents and flame temperature on particle size, morphology, and photoluminescence intensity were investigated. The results showed that flame synthesis using ethanol solution could produce nanoparticles with better homogeneity, smoother surface structure, and stronger p...