Chemical and Morphological Characterization of Magnetron Sputtered at Different Bias Voltages Cr-Al-C Coatings
نویسندگان
چکیده
MAX phases (M = transition metal, A = A-group element, and X = C/N) are of special interest because they possess a unique combination of the advantages of both metals and ceramics. Most attention is attracted to the ternary carbide Cr2AlC because of its excellent high-temperature oxidation, as well as hot corrosion resistance. Despite lots of publications, up to now the influence of bias voltage on the chemical bonding structure, surface morphology, and mechanical properties of the film is still not well understood. In the current study, Cr-Al-C films were deposited on silicon wafers (100) and Inconel 718 super alloy by dc magnetron sputtering with different substrate bias voltages and investigated using Scanning Electron Microscopy (SEM), X-ray Photoelectron Spectroscopy (XPS), X-ray Diffraction (XRD), Atomic Force Microscopy (AFM), and nanoindentation. Transmission Electron Microscopy (TEM) was used to analyze the correlation between the growth of the films and the coating microstructure. The XPS results confirm the presence of Cr2AlC MAX phase due to a negative shift of 0.6-0.9 eV of the Al2p to pure aluminum carbide peak. The XRD results reveal the presence of Cr2AlC MAX Phase and carbide phases, as well as intermetallic AlCr2. The film thickness decreases from 8.95 to 6.98 µm with increasing bias voltage. The coatings deposited at 90 V exhibit the lowest roughness (33 nm) and granular size (76 nm) combined with the highest hardness (15.9 GPa). The ratio of Al carbide to carbide-like carbon state changes from 0.12 to 0.22 and correlates with the mechanical properties of the coatings. TEM confirms the columnar structure, with a nanocrystalline substructure, of the films.
منابع مشابه
The Effect of Substrate Temperature and Biasing on Physical-Properties and Corrosion Resistance of CrN/Al 5083 Coatings
Aluminum alloys such as Al 5083 have primary potential for lightweight structural application in automotive and aerospace industries. This paper addresses the mechanical and tribological properties and corrosion resistance of chromium nitride coatings deposited on Al 5083 that can be used for development of applications of aluminum 5083 alloy. The CrN coatings of 1 μm thickness were deposited b...
متن کاملThe Effect of Substrate Temperature and Biasing on Physical-Properties and Corrosion Resistance of CrN/Al 5083 Coatings
Aluminum alloys such as Al 5083 have primary potential for lightweight structural application in automotive and aerospace industries. This paper addresses the mechanical and tribological properties and corrosion resistance of chromium nitride coatings deposited on Al 5083 that can be used for development of applications of aluminum 5083 alloy. The CrN coatings of 1 μm thickness were deposited b...
متن کاملEffect of Substrate Bias Voltage and Ti Doping on the Tribological Properties of DC Magnetron Sputtered MoSx Coatings
Molybdenum disulfide (MoS2) is one of the most widely used solid lubricants. In this work, composite MoSx/Ti coatings were deposited by direct-current magnetron sputter ion plating onto plain carbon steel substrates. The MoSx/Ti ratio in the coatings was controlled by sputtering the composite targets. The composition, microstructure, and mechanical properties of the coatings were explored using...
متن کاملA Study of the Tribological Properties of Sputter-deposited MoSX/Cr Coatings
In this investigation, MoSx/Cr coatings were deposited by direct-current magnetron sputter onto Ck45 (AISI 1045) plain carbon steel substrates. The MoSx/Cr ratio in the coatings was controlled by sputtering the composite targets. The chemical characterization was performed using EDX (energy dispersive X-ray analysis); the structural characterization was accomplished by X-ray diffraction (XRD) s...
متن کاملHigh temperature properties of the Cr-Nb-Al-N coatings with increasing Al contents
Cr-Nb-Al-N coatings with Al content from 0 to 12 at.% were deposited by d.c. reactive magnetron sputtering. The coatings were annealed in protective atmosphere at 800 and 900 o C for 1h and exposed to air at 800, 900 and 1200 o C for different times. The chemical composition, structure, microstructure, hardness and adhesive/cohesive strength of the coatings, in as-deposited and annealed conditi...
متن کامل