Clinical Marginal and Internal Adaptation of Maxillary Anterior Single All-Ceramic Crowns and 2-year Randomized Controlled Clinical Trial.

نویسندگان

  • Aslı Akın
  • Suna Toksavul
  • Muhittin Toman
چکیده

PURPOSE The aims of this randomized-controlled clinical trial were to compare marginal and internal adaptation of all-ceramic crowns fabricated with CAD/CAM and heat-pressed (HP) techniques before luting and to evaluate the clinical outcomes at baseline and at 6, 12, and 24 months after luting. MATERIALS AND METHODS Fifteen CAD/CAM (CC) and 15 HP all-ceramic crowns were placed in 15 patients. A silicone replica was obtained to measure marginal and internal adaptation of each all-ceramic crown before luting, and they were sectioned buccolingually and mesiodistally. Marginal and internal adaptations were measured using computerized light microscope at 40× magnification. Clinical evaluations took place at baseline (2 days after luting) and at 6, 12, and 24 months after luting. Replica scores were analyzed with Mann-Whitney U and Student's t-test (α = 0.05). Survival rate of crowns was determined using Kaplan-Meier statistical analysis. RESULTS The median marginal gap for the CC group was 132.2 μm and was 130.2 μm for the HP group. The mean internal adaptation for the CC group was 220.3 ± 51.3 μm and 210.5 ± 31 μm for the HP group. There were no statistically significant differences with respect to marginal opening (Mann-Whitney U test; p = 0.95) and internal adaptation (Student's t-test; p = 0.535) between the 2 groups. Based on modified Ryge criteria, 100% of the crowns were rated satisfactory during the 2-year period. CONCLUSION In this in vivo study, CAD/CAM and HP all-ceramic crowns exhibited similar marginal and internal adaptations. A 100% success rate was recorded for the 15 CAD/CAM and for the 15 HP all-ceramic crowns during the 2-year period.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Effect of Different Finishing Lines on the Marginal Fitness of Full Contour Zirconia and Glass Ceramic CAD/CAM Crowns (An in-vitro study)

Purpose: The aim of this study was to evaluate the effect of two gingival finishing lines (90° shoulder and deep chamfer) on the marginal fitness of two types of full anatomic all-ceramic crowns; zirconia crowns (Zikonzhan) and glass ceramic crowns (IPS e-max CAD) milled with CAD/CAM system. Materials and Methods: Two dentoform teeth of left maxillary first molar were prepared with chamfer fini...

متن کامل

Marginal and internal adaptation of zirconium dioxide ceramic copings and crowns with different finish line designs.

The present study evaluated the marginal and internal adaptation of single-tooth zirconium dioxide (ZrO2) ceramic copings or crowns with three different finish line designs. Twenty-four steel dies were prepared for maxillary central incisor crowns with the following finish line designs: shoulder (S), rounded shoulder (RS), and chamfer (C) preparations. Twenty-four standardized ZrO2 ceramic copi...

متن کامل

The evaluation and comparison of marginal adaptation in metal ceramic and all ceramic restorations fabricated by two methods: CAD/CAM and conventional

Introduction: Marginal fit is a key factor for long term clinical success through any dental restorations. Poor marginal adaptation causes cement dissolution. This can lead to dental caries, gingival irritation, periodontal diseases, and finally treatment failure. The aim of this study was measurement and comparison of marginal gap quantities in metal ceramic and all ceramic dental restorations...

متن کامل

Cad/cam Zirconia vs. Slip-cast Glass-infiltrated Alumina/zirconia All-ceramic Crowns: 2-year Results of a Randomized Controlled Clinical Trial

The aim of this randomized controlled clinical trial was to compare the early clinical outcome of slip-cast glass-infiltrated Alumina/Zirconia and CAD/CAM Zirconia all-ceramic crowns. A total of 30 InCeram Zirconia and Cercon Zirconia crowns were fabricated and cemented with a glass ionomer cement in 20 patients. At baseline, 6-month, 1-year, and 2-year recall appointments, Californian Dental A...

متن کامل

Adhesively restored anterior maxillary dentitions affected by severe erosion: up to 6-year results of a prospective clinical study.

UNLABELLED In case of severe dental erosion, the maxillary anterior teeth are often particularly affected. Restoring such teeth conventionally (ie, crowns) would frequently involve elective endodontic therapy and major additional loss of tooth structure. A novel, minimally invasive approach to restore eroded teeth has been developed and is currently being tested in the form of a prospective cli...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of prosthodontics : official journal of the American College of Prosthodontists

دوره 24 5  شماره 

صفحات  -

تاریخ انتشار 2015