Low-Temperature Carbothermic Reduction of Indonesia Nickel Lateritic Ore with Sub-Bituminous Coal

نویسندگان

  • I Setiawan
  • S Harjanto
چکیده

In this work, the experiment was conducted to investigate the effect of temperature and sub-bituminous coal on upgrading nickel laterites ores by carbothermic reduction. The reduction was carried out in the muffle furnace at a temperature ranging of 800-1100 o C. The produced calcine from reduction step was grounded in vibrating mill, mixed with water and passed on a magnetic separator to separate nickel concentrates from the tailing. The experimental results showed that the concentrate with highest nickel grade was produced at temperature 1000 o C. The nickel grade on concentrate was 5.0 %, with the recovery of nickel was 80.6 %.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

KINETICS OF CARBOTHERMIC REDUCTION OF AN IRANIAN CELESTITE ORE

Two commercial methods are used for the production of strontium carbonate:1) Direct conversion of Celsetite to strontium carbonate by hot sodium carbonate,2) Carbothermic reduction of celestite with coal followed by water leaching of strontium sulfide(SrS) and its conversion to strontium carbonate.The present study has been made on the carbothermic reduction of celestite ores of Varamin (Iran) ...

متن کامل

An Investigation on the Reduction of Iron Ore Pellets in Fixed Bed of Domestic Non–Coking Coals

In this study, the isothermal reduction of iron oxide pellets, made of Iranian Chadormalo, Gole-gohar, and Sangan iron ores, was investigated in the temperature range of 900-1100°C. Tabas, Pabdana, Babnizoo, Karmozd, and Shahrood domestic coals were used as reductants. Parametric studies were performed and the effects of such factors as temperature, average particle size of iron ore and coal fi...

متن کامل

Microbial Treatment of Lateritic Ni-ore for Iron Beneficiation and Their Characterization

Th is study aims at studying effect of anaerobic dissimilatory iron (III) reducing bacterial consortium on different phases of iron present in lateritic n ickel ore. Such conversion in lateritic nickel ore are helpful in better recovery of sorbed metal values like Ni and Co by subsequent bioleaching or acid leaching. Here properties of thermally and microbially reduced lateritic nickel ore are ...

متن کامل

An Investigation on the Reduction of Iron Ore Pellets in Fixed Bed of Domestic Non–Coking Coals

In this study, the isothermal reduction of iron oxide pellets, made of Iranian Chadormalo, Gole-gohar, and Sangan iron ores, was investigated in the temperature range of 900-1100°C. Tabas, Pabdana, Babnizoo, Karmozd, and Shahrood domestic coals were used as reductants. Parametric studies were performed and the effects of such factors as temperature, average particle size of iron ore and coal fi...

متن کامل

EFFECT OF MECHANICAL ACTIVATION ON CARBOTHERMIC SYNTHESIS OF TITANIUM CARBIDE FROM ILMENITE CONCENTRATE

The synthesis of advanced materials from low cost minerals concentrates is a new field of study that has great potential applications. In this paper, the effect of milling time on the temperature of initiation and amount of carbothermic reduction of ilmenite has been investigated. The stoichiometric molar ratio (1:4) of ilmenite to graphite was mixed and mechanically activatedfor 30-70 hours at...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2017