his article describes the properties, advances and shortcomings of glass-ionomer cement as a restorative material. The adhesion of glass-ionomer to tooth structure is less technique sensitive than composite resins and its quality increases with time. Therefore glass-ionomer might turn out to the more reliable restorative material in minimal invasive dentistry based on adhesive techniques. Uniterms: Glass ionomer cements adhesion; Minimum intervention; Sealant restorations.
منابع مشابه
Compressive and Diametral Tensile Strength of Glass Ionomer Cements Resistência À Compressão E À Tração Diametral De Cimentos De Ionômero De Vidro
1DDS, MSc, PhD, Graduate Student, Department of Operative Dentistry, Bauru Dental School, University of São Paulo, Brazil. 2DDS, MSc, Graduate Student, Department of Operative Dentistry, Bauru Dental School, University of São Paulo, Brazil. 3Undergraduate Student of Bauru Dental School, University of São Paulo, Brazil. 4Associate Professor of Operative Dentistry, Dean of Bauru Dental School, Un...
متن کاملDiametral Tensile Strength and Water Sorption of Glass-ionomer Cements Used in Atraumatic Restorative Treatment Resistência À Tração Diametral E Sorção De Água De Cimentos De Ionômero De Vidro Usados No Tratamento Restaurador Atraumático
he purposes of this study were to evaluate the diametral tensile strength and the water sorption of restorative (Fuji IX and Ketac Molar) and resin-modified glass-ionomer luting cements (ProTec Cem, Fuji Plus and Vitremer) mixed at both manufacturer and increased powder: liquid ratio, for their use in the Atraumatic Restorative Treatment. A conventional restorative glass-ionomer (Ketac Fil) was...
متن کاملBiological Compatibility of Some Types of Endodontic Calcium Hydroxide and Glass Ionomer Cements Biocompatibilidade De Alguns Tipos De Cimento Endodôntico À Base De Hidróxido De Cálcio E Cimentos De Ionômero De Vidro
1PhD Professor, Department of Restorative Dentistry, São José dos Campos Dental School, UNESP, São José dos Campos, SP, Brazil. 2Chairman Professor, Department of Restorative Dentistry, Araraquara Dental School, UNESP, Araraquara, SP, Brazil. 3Chairman Professor, Department of Pathology, Bauru Dental School, University of São Paulo, USP, Bauru, SP, Brazil. 4Graduate student of Restorative Denti...
متن کاملEvaluation of Marginal Microleakage and Depth of Penetration of Glass Ionomer Cements Used as Occlusal Sealants Avaliação Da Microinfiltração Marginal E Profundidade De Penetração Dos Cimentos De Ionômero De Vidro Utilizados Como Selantes Oclusais
1DDS, MSc, PhD, student of the Department of Pediatric Dentistry of Bauru School, University of São Paulo, São Paulo, Brazil, and Assistant Professor of the Discipline of Pediatric Dentistry of the State University of Maringá, Maringá-PR, Brazil. 2DDS, MSc, PhD, Assistent Professor of the Discipline of Pediatric Dentistry of the Center for Superior Teaching, Maringá-PR, Brazil. 3DDS, MSc, PhD, ...
متن کاملEffect of One-bottle Adhesive Systems on the Fluoride Release of a Resin-modified Glass Ionomer Efeito Dos Sistemas Adesivos De Frasco Único Na Liberação De Flúor De Um Cimento De Ionômero De Vidro Modificado Por Resina
dhesive systems associated to resin-modified glass ionomer cements are employed for the achievement of a higher bond strength to dentin. Despite this benefit, other properties should not be damaged. This study aimed at evaluating the short-time fluoride release of a resin-modified glass ionomer cement coated with two one-bottle adhesive systems in a pH cycling system. Four combinations were inv...
متن کامل