Deposition and Characterization of Si-Doped Diamond Films Using Tetraethoxysilane onto a WC-Co Substrate

نویسندگان

  • Jianguo Zhang
  • Xia Ji
  • Jinsong Bao
  • Xiaohu Zheng
  • Maria Miritello
چکیده

Silicon-doped (Si-doped) diamond films were deposited on a Co-cemented tungsten carbide (WC-Co) substrate using the hot filament chemical vapor deposition (HFCVD) method with a mixture of acetone, tetraethoxysilane (TEOS), and hydrogen as the recant source. The as-deposited doped diamond films were characterized with field emission scanning electron microscopy (FE-SEM), Raman spectrum, and X-ray diffraction (XRD). Furthermore, Rockwell C indentation tests were conducted to evaluate the adhesion of the Si-doped diamond films grown on the WC-Co substrate. The results demonstrated that the silicon concentration in the reactant source played an important role in the surface morphology and adhesion of diamond films. The size of diamond grain varied from 3 μm to 500 nm with silicon concentration increasing from 0 to 1.41 atom %. When the silicon concentration rose to 1.81 atom %, the grain size became bigger than that of the lower concentration. The ratio of diamond peak {220}/{111} varied with different silicon concentrations. Raman study features revealed high purity of as-deposited diamond films. The Raman spectra also demonstrated the presence of silicon in the diamond films with Si–Si, Si–C and Si–O bonds. Si-doped diamond films with strong adhesive strength on the WC-Co substrate was beneficial for diamond films applied on cutting tools and wear resistance components.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fabrication of Copper and Iron Nano/Micro Structures on Semiconducting Substrate and Their Electrical Characterization

In this paper, we have studied the electrical properties of the randomly distributed metallic (Co and Fe) nano/ micro wires on Silicon substrate. Deposition was carried out potentiostatically into the pores of the track-etch polycarbonate membrane spin coated onto the Si substrate. Spin coated films were irradiated with 150MeV Ni (+11) ions at a fluence of 8E7 ions/cm2, followed by UV irradiati...

متن کامل

Simulation of Fabrication toward High Quality Thin Films for Robotic Applications by Ionized Cluster Beam Deposition

The most commonly used method for the production of thin films is based on deposition of atoms or molecules onto a solid surface. One of the suitable method is to produce high quality metallic, semiconductor and organic thin film is Ionized cluster beam deposition (ICBD), which are used in electronic, robotic, optical, optoelectronic devices. Many important factors such as cluster size, cluster...

متن کامل

STUDY OF CHARACTERIZATION AND CORROSION RESISTANCE OF NIP/NANO-DIAMOND ELECTROLESS COMPOSITE DEPOSITION

Ni-P Electroless coatings provide appropriate resistance to wear and corrosion. Co-deposition of particles between layers can improve their properties, especially general corrosion and erosion-corrosion behavior by means of nano diamond as reinforcing particles. In this study Ni-P/nano diamond composite deposition were deposited on steel substrate. Structure of the coatings and corrosion r...

متن کامل

Boron nitride thin films deposited by RF plasma reactive pulsed laser ablation as interlayer between WC–Co hard metals and CVD diamond films

Thin films of boron nitride have been obtained by reactive pulsed laser ablation of a boron target in the presence of a 13.56 MHz radio frequency nitrogen plasma. The films have been deposited at several substrate temperatures, using the on-axis configuration, on WC–Co cutting tools, after Co removal by chemical etching (HClyHNO or HFyHNO ). Diamond polycrystalline 3 3 films of increasing thick...

متن کامل

Effect of Boron-Doped Diamond Interlayer on Cutting Performance of Diamond Coated Micro Drills for Graphite Machining

Thin boron doped diamond (BDD) film is deposited from trimethyl borate/acetone/hydrogen mixture on Co-cemented tungsten carbide (WC-Co) micro drills by using the hot filament chemical vapor deposition (HFCVD) technique. The boron peak on Raman spectrum confirms the boron incorporation in diamond film. This film is used as an interlayer for subsequent CVD of micro-crystalline diamond (MCD) film....

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2016