Slippage of Steel in High and Normal Strength Concrete

نویسندگان

  • K. Ahmed
  • Z. A. Siddiqi
  • M. Yousaf
چکیده

Composite action of any reinforced concrete member is only possible if sufficient bond strength exists between steel reinforcing bars and concrete, which can adequately transfer shear stress between them. Bond strength is a function of compressive strength of concrete and hence high strength concrete has higher bond strength [1-2]. Therefore required development length can be reduced. In order to investigate the effect of development length on bond stress and slip relationships, experimental investigation was carried out. In this experimentation 24 pull-out samples of high strength concrete and normal strength concrete were casted and tested. The results of this investigation revealed that by increasing the development length from 5db to 10db bond strength increases for both high and normal strength concrete as shown in Figure 11, 12 and 13. However incase of normal strength concrete increase in bond strength is more compared to that in high strength concrete as it is clear from Figure 11 and Figure 13. The increase in bond strength is observed even at 10db development length but the extent is less for 19 mm than 16 mm bars as shown in Figure 12 and Figure 13. This is in agreement with the earlier findings of Chen et al [3] and Harajli et al [1]. However incase of HSC the total slippage at 10db is 50% greater than at 5db. This may be due to the fact that more no of concrete keys participate in resisting the slippage.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of the Concrete Strength on the Concrete-Steel Bond in Concrete Filled Steel Tubes

In this study, the concrete-steel bond strength of concrete filled cylindrical steel tubes has been experimentally investigated. 22 short, high strength and normal concrete filled circular steel tubes were tested. Push-out test was carried out as the common method to evaluate the bond carrying capacity. Four different concrete mixes were used in preparing the specimens. The steel tubes were w...

متن کامل

Flexural Performance of High-strength Prestressed Concrete-encased Concrete-filled Steel Tube Sections

The sections composed of concrete and steel, which include concrete-encased concrete-filled tubes, generally have defects due to the low tensile strength of concrete. Therefore, an appropriate method was used for the combination of concrete-filled tubes (CFT) and prestressing strands which is encased in concrete. The conventional design guidelines are commonly developed for materials with norma...

متن کامل

CORROSION BEHAVIOR OF ZINC COATED STEEL REBAR IN HIGH-STRENGTH REINFORCED CONCRETE

A large number of reinforced concrete structures subjected to chloride ions. Two basicapproaches for preventing corrosion of reinforcing steel embedded in concrete are: Increasing theconsolidation of concrete and using different coating on rebars. In present research steel rebarsare coated in different ways: a) 40 µm of zinc electroplated on steel rebar b) Zinc powder withepoxy paste (zinc rich...

متن کامل

Mechanical Behavior of Hybrid Fiber Reinforced High Strength Concrete with Graded Fibers

Brittleness, which was the inherent weakness in High Strength Concrete (HSC), can be avoided by reinforcing the concrete with discontinuous fibers. Reinforcing HSC with more than one fiber is advantageous in an overall improvement of the mechanical performance of the composite. In this experimental study, Hybrid Fiber Reinforced High Strength Concrete (HyFR-HSC) mixes were formed by blending si...

متن کامل

Effect of Impressed Current on Bond Strength Between Steel Rebar and Concrete

The deterioration of bond strength between reinforcing steel and concrete as a result of impressed cathodic current with respect to the exposure time was investigated. A current in the magnitude of 3ma/ft2 (based on reinforcing rebar area) was used for a period of five years. Chemical analyses for sodium (Na+), potassium (K+) and chloride (Cl-) ions in concrete cylinders were performed as a fun...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2007