A B S T R A C T Various analogies have recently been proposed for comparing the stress fields induced in fretting fatigue contact situations, with those of a crack and a sharp or a rounded notch, resulting in a degree of uncertainty over which model is most appropriate in a given situation. However, a simple recent approach of Atzori–Lazzarin for infinite-life fatigue design in the presence of a geometrical notch suggests a corresponding unified model also for fretting fatigue (called Crack-Like Notch Analogue model) considering only two possible behaviours: either 'crack-like' or 'large blunt notch.' In a general fretting fatigue situation, the former condition is treated with a single contact problem corresponding to a Crack Analogue model; the latter, with a simple peak stress condition (as in previous Notch Analogue models), simply stating that below the fatigue limit, infinite life is predicted for any size of contact. In the typical situation of constant normal load and in phase oscillating tangential and bulk loads, both limiting conditions can be readily stated. Not only is the model asymptotically correct if friction is infinitely high or the contact area is very small, but also remarkably accurate in realistic conditions, as shown by excellent agreement with Hertzian experimental results on Al and Ti alloys. The model is useful for preliminary design or planning of experiments reducing spurious dependences on an otherwise too large number of parameters. In fact, for not too large contact areas ('crack-like' contact) no dependence at all on geometry is predicted, but only on three load factors (bulk stress, tangential load and average pressure) and size of the contact. Only in the 'large blunt notch' region occurring typically only at very large sizes of contact, does the size-effect disappear, but the dependence is on all other factors including geometry. a = notch or crack half-width (i.e., contact half-width) a 0 = El Haddad intrinsic crack size K f = fatigue strength reduction factor K ff = K f in the region of crack-like fretting fatigue notch behaviour K ft = K f in the region of blunt fretting fatigue notch behaviour K t = elastic stress concentration factor K th = threshold value of the stress intensity factor range Y = geometric or fretting fatigue shape factor σ = range of the gross nominal stress σ l = plain specimen fatigue limit (in terms of stress range) Fretting was originally …

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Dc Electrical Potential Method for the Measumment of Fretting Cracks

As fretting fatigue cracks are initiated at an early stage of life, the fretting fracture process is dominated by the stable growth of cracks. Hence the measurement of crack length is very important. This paper demonstrates the suitability of the DC potential drop technique for the measurement of fretting cracks. A calibration has been established for monitoring crack growth in BS L65 copper al...

متن کامل

NUMERICAL INVESTIGATION OF CRACK ORIENTATION IN THE FRETTING FATIGUE OF A FLAT ROUNDED CONTACT

The growth of slant cracks by fretting fatigue of a half plane in contact with a flat rounded pad was studied. The mode I and mode II stress intensity factors for cracks of various lengths and directions were calculated using the semi-analytical method of the distribution of dislocations, and their cumulative effect on the crack growth was investigated using the strain energy density criterion....

متن کامل

Fretting Fatigue with Cylindrical-On-Flat Contact: Crack Nucleation, Crack Path and Fatigue Life

Fretting fatigue experiments and finite element analysis were carried out to investigate the influence of cylindrical-on-flat contact on crack nucleation, crack path and fatigue life of medium-carbon steel. The location of crack nucleation was predicted using the maximum shear stress range criterion and the maximum relative slip amplitude criterion. The prediction using the maximum relative sli...

متن کامل

1 Development of a Fretting - Fatigue Mapping concept : Impact of material properties and Surface treatments

Fretting fatigue induced by combined localized cyclic contact motion and external bulk fatigue loadings may result in premature and dramatic failure of the contacting components. Depending on fretting and fatigue loading conditions, crack nucleation and possibly crack propagation can be activated. This paper proposes a procedure for estimating these two damage thresholds. The crack nucleation b...

متن کامل

Development of a Fretting - Fatigue Mapping concept : Impact of material properties and Surface treatments

Fretting fatigue induced by combined localized cyclic contact motion and external bulk fatigue loadings may result in premature and dramatic failure of the contacting components. Depending on fretting and fatigue loading conditions, crack nucleation and possibly crack propagation can be activated. This paper proposes a procedure for estimating these two damage thresholds. The crack nucleation b...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2003