Volcanic sintering: Timescales of viscous densification and strength recovery

نویسندگان

  • Jérémie Vasseur
  • Fabian B Wadsworth
  • Yan Lavallée
  • Kai-Uwe Hess
  • Donald B Dingwell
چکیده

[1] Sintering and densification are ubiquitous processes influencing the emplacement of both effusive and explosive products of volcanic eruptions. Here we sinter ash-size fragments of a synthetic National Institute of Standards and Technology viscosity standard glass at temperatures at which the resultant melt has a viscosity of ∼108-109 Pa.s at 1bar to assess sintering dynamics under near-surface volcanic conditions. We track the strength recovery via uniaxial compressive tests. We observe that volcanic ash sintering is dominantly time dependent, temperature dependent, and grain size dependent and may thus be interpreted to be controlled by melt viscosity and surface tension. Sintering evolves from particle agglutination to viscous pore collapse and is accompanied by a reduction in connected porosity and an increase in isolated pores. Sintering and densification result in a nonlinear increase in strength. Micromechanical modeling shows that the pore-emanated crack model explains the strength of porous lava as a function of pore fraction and size.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Gravitational Effects on Distortion in Sintering

During sintering a powder compact gains strength through low-temperature interparticle bonding, usually induced by solid-state surface diffusion, followed by further strength contributions from high-temperature densification. In cases where a liquid phase forms, sintering densification is accelerated and shape retention is sustained while open pores remain and contribute capillary forces. Unfor...

متن کامل

Effect of Silicon Carbide and graphite additives on the pressureless Sintering mechanism and microstructural characteristics of Ultra-High Temperature ZrB2 Ceramics Composites

The effect of SiC content, additives, and process parameters on densification and microstructural properties of pressureless sintered ZrB2– (1–10 wt %) SiC particulate composites have been studied. The ZrB2–SiC composite powders mixed by Spex mixer with 1-2wt% C (added as graphite powder) and CMC have been cold-compacted and sintered in argon environment in the temperature range of 1800–2100ºC ...

متن کامل

Evaluation of Heterogeneous Densification, Anisotropic Shrinkage and Rheological Behavior of Ceramic Materials during Liquid Phase Sintering by Numerical-Experimental Procedure

The effective shear and bulk viscosity, as well as dynamic viscosity, describe the rheological properties of the ceramic body during the liquid phase sintering process. The rheological parameters depend on the physical and thermo-mechanical characteristics of the material such as relative density, temperature, grain size, diffusion coefficient, and activation energy. Thermal behavior of the cer...

متن کامل

Finite element simulation of pyroplastic deformation, anisotropic shrinkage and heterogeneous densification for ceramic materials during liquid phase sintering process

Pyroplastic deformation is a distortion of the ceramic shape during the sintering process. It occurs because the flow of the vitreous phase at high temperature and the applied stress due to the weight of the product during sintering process. The aim of this paper deals with describing a numerical-experimental method to evaluate the pyroplastic deformation, to predict the anisotropic shrinkage a...

متن کامل

DENSIFICATION AND MICROSTRUCTURE CHARACTERISTICS OF A PREALLOYED ALPHA BRASS POWDER PROCESSED BY LIQUID PHASE SINTERING

The rapidly solidified prealloyed alpha brass powder with a size range of 40 to 100 μm produced by water atomization process was consolidated using liquid phase sintering process. The relationships between sintering temperature, physic-mechanical properties and microstructural characteristics were investigated. Maximum densification was obtained at 930 °C, under 600 MPa compacting pressure,...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 40  شماره 

صفحات  -

تاریخ انتشار 2013