Shear bond resistance and enamel surface comparison after the bonding and debonding of ceramic and metallic brackets

نویسندگان

  • José Maurício da Rocha
  • Marco Abdo Gravina
  • Marcio José da Silva Campos
  • Cátia Cardoso Abdo Quintão
  • Carlos Nelson Elias
  • Robert Willer Farinazzo Vitral
چکیده

OBJECTIVE To evaluate, in vitro, the shear bond strength presented by three brands of polycrystalline ceramic brackets and one brand of metallic bracket; verify the adhesive remnant index (ARI) after the tests, and analyze, through scanning electron microscopy (SEM) the enamel surface topography after debonding, detecting the release of mineral particles. METHODS Sixty bovine lower incisors were used. Three ceramic brackets (Allure®, InVu®, and Clarity®) and one metallic bracket (Geneus®) were bonded with Transbond XT®. Kruskal-Wallis's test (significance level set at 5%) was applied to the results of shear bond and ARI. Mann Whitney's test was performed to compare the pairs of brackets in relation to their ARI. Brown-Forsythe's test (significance level set at 5%) was applied to the results of enamel chemical composition. Comparisons between groups were made with Games-Howell's and the Post-hoc tests. RESULTS No statistically significant difference was observed in relation to the shear bond strength loads. Clarity® brackets were the most affected in relation to the surface topography and to the release of mineral particles of enamel (calcium ions). CONCLUSIONS With regard to the ARI, there was a prevalence of score 4 (40.4%). As for enamel surface topography, the Geneus® bracket was the only one which did not show superficial tissue loss. The InVu® and Clarity® ones showed cohesive fractures in 33.3% and the Allure® in 50%, the latter being the one that presented most fractures during removal.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Comparison between self-etching and conventional primers in repeated bracket bonding

Background and Aim: This study aimed to evaluate the effect of repeated bonding by self-etching primers (SEPs) and a conventional phosphoric acid-etchant on shear bond strength (SBS), adhesive remnant index (ARI), and enamel morphology at different debonding time points. Materials and Methods: In this experimental study, 120 premolars were randomly divided into six groups of 20. In the first t...

متن کامل

Shear bond strength of metallic and ceramic brackets using color change adhesives.

OBJECTIVE To determine the shear bond strength of orthodontic brackets using color change adhesives that are supposed to aid in removing excess of bonding material and compare them to a traditional adhesive. METHODS Ninety metallic and ninety ceramic brackets were bonded to bovine incisors using two color change adhesives and a regular one. A tensile stress was applied by a universal testing ...

متن کامل

In vitro Effects of a Neutral Fluoride Agent on Shear Bond Strength and Microleakage of Orthodontic Brackets

Introduction: This study aimed to evaluate the effect of pretreatment with a neutral fluoride agent on shear bond strength (SBS) and microleakage of orthodontic brackets, and to investigate any significant relationship between SBS and microleakage. Methods: Forty intact premolars were selected and randomly divided into 2 groups. Group 1 served as the control, while group 2 underwent treatment w...

متن کامل

Shear Bond Strength of Metallic and Ceramic Brackets Bonded with Two-step and Three-step Light Cure Adhesives

  Background and purpose: The bonding process is highly important in orthodontic treatment for its fast speed. The purpose of this study was to compare the shear bond strength of ceramic and metallic brackets between three stage (transbondTM XT) and two stage (GC ortho connectTM) light cure composites. Materials and methods: In this experimental study, 80 maxillary and mandibular first and sec...

متن کامل

Comparison of shear bond strength of the stainless steel metallic brackets bonded by three bonding systems

Introduction: In orthodontic treatment, it is essential to establish a satisfactory bond between enamel and bracket. After the self-etch primers (SEPs) were introduced for the facilitation of bracket bonding in comparison to the conventional etch-and-bond system, multiple studies have been carried out on their shear bond strengths which have yielded different results. This study was aimed at co...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 19  شماره 

صفحات  -

تاریخ انتشار 2014