Strength of joints produced by transient liquid phase bonding in the Cu–Sn system

نویسندگان

  • N. S. Bosco
  • F. W. Zok
چکیده

The paper focuses on the strength and toughness of joints produced by transient liquid phase (TLP) bonding in the Cu–Sn system. It is motivated by potential applications of TLP bonding in attachment of high-temperature wide bandgap devices to ceramic substrates. Model test specimens suitable for mechanical testing are developed, utilizing substrates of oxide dispersion strengthened copper. Three microstructural conditions are probed: a uniform layer of the d intermetallic phase (Cu41Sn11), a two-phase microstructure comprising the d-phase and a dispersion of ductile (Cu) particles, and a uniform Cu solid solution. Notched and unnotched bend tests are used to ascertain strength and toughness. The d-phase exhibits a reasonably high strength (300 MPa), but low toughness ( 5 MPapm). Addition of (Cu) particles increases both the strength and the toughness by about 30% (400 MPa and 7 MPa p m, respectively). These property enhancements are rationalized on the basis of existing models of ductile phase toughening. The conversion of the intermetallic to Cu solid solution leads to a decrease in strength (to 200 MPa), but an increase in toughness (to 13 MPa p m). The latter trends appear to be a consequence of the reduction in the flow stress of the joint material. Additionally, the conversion to (Cu) is accompanied by the formation of voids, predominantly near the prior boundary between the d-phase and the adjoining Cu. The voids likely diminish the joint properties, relative to the intrinsic values associated with the defect-free copper solid solution. 2005 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Temperature and Time on the Joint Properties of AISI420 Steel to SAF2507 Steel Produced by Transient Liquid Phase Process

In this research, the effect of temperature and time on the properties of AISI420/SAF2507 dissimilar joint produced by transient liquid phase bonding process was investigated. A BNi-2 interlayer with 25 μm thickness was inserted between two dissimilar steel samples. The bonding process was performed at 1050 oC and 1100 oC for different bonding times. The microstructures of the joints were studi...

متن کامل

The effect of bonding temperature on the characteristics of TLP bonded joints in AISI 2205/BNi-3/AISI 2205 assembly

In the present study, the transient liquid phase bonding of AISI 2205 dual phase stainless steel with amorphous BNi-3 interlayer was carried out. Based on the initial experimental and analytical studies, the parameters of temperature and bonding time were determined. In order to investigate the effect of bonding temperature on the microstructural changes of the joint, bonding was performed in t...

متن کامل

The effect of bonding temperature on the characteristics of TLP bonded joints in AISI 2205/BNi-3/AISI 2205 assembly

In the present study, the transient liquid phase bonding of AISI 2205 dual phase stainless steel with amorphous BNi-3 interlayer was carried out. Based on the initial experimental and analytical studies, the parameters of temperature and bonding time were determined. In order to investigate the effect of bonding temperature on the microstructural changes of the joint, bonding was performed in t...

متن کامل

Investigation of the mechanical properties and microstructure of the Ti-6Al-4V to Al2024 joint fabricated by successive- stage transient liquid phase (S-TLP) method

The aim of this study is investigation of TLP variables on microstructure and mechanical properties of Al2024 to Ti-6Al-4V bonding for TLP joint. For this purpose, the sheets were prepared with dimension of 130×32×3 mm from Ti-6Al-4V and Al2024 alloys and 50µm thick Sn-5.3Ag-4.2Bi foil as interlayer. Sn-5.3Ag-4.2Bi foil prepared with dimension of 32×25 mm. Two alloys was joint together by proce...

متن کامل

The effect of bonding temperature on the microstructure and mechanical properties of 939 super alloy by transient liquid phase bonding method

In this research, the effect of bonding temperature on the microstructure and mechanical properties of Inconel 939 super alloy by transient liquid phase bonding method. For this purpose, the middle layer of MBF20 with a thickness of 50 microns and three temperatures of 1060 °C, 1120 °C, 1180 °C and a time of 45 minutes have been used. In order to evaluate the microstructure, a scanning electron...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2005