Effects of core characters and veneering technique on biaxial flexural strength in porcelain fused to metal and porcelain veneered zirconia
نویسندگان
چکیده
PURPOSE The purpose of this study was to assess the impact of the core materials, thickness and fabrication methods of veneering porcelain on prosthesis fracture in the porcelain fused to metal and the porcelain veneered zirconia. MATERIALS AND METHODS Forty nickel-chrome alloy cores and 40 zirconia cores were made. Half of each core group was 0.5 mm-in thickness and the other half was 1.0 mm-in thickness. Thus, there were four groups with 20 cores/group. Each group was divided into two subgroups with two different veneering methods (conventional powder/liquid layering technique and the heat-pressing technique). Tensile strength was measured using the biaxial flexural strength test based on the ISO standard 6872:2008 and Weibull analysis was conducted. Factors influencing fracture strength were analyzed through three-way ANOVA (α≤.05) and the influence of core thickness and veneering method in each core materials was assessed using two-way ANOVA (α≤.05). RESULTS The biaxial flexural strength test showed that the fabrication method of veneering porcelain has the largest impact on the fracture strength followed by the core thickness and the core material. In the metal groups, both the core thickness and the fabrication method of the veneering porcelain significantly influenced on the fracture strength, while only the fabrication method affected the fracture strength in the zirconia groups. CONCLUSION The fabrication method is more influential to the strength of a prosthesis compared to the core character determined by material and thickness of the core.
منابع مشابه
Shear bond strength of veneering porcelain to porous zirconia.
In this study, two types of porous zirconia and dense zirconia were used. The flexural strength of non-layered zirconia specimens and those of the layered zirconia specimens with veneering porcelain were examined. Furthermore, the shear bond strength of veneering porcelain to zirconia was examined. The flexural strength of the non-layered specimens was 1,220 MPa for dense zirconia and 220 to 30...
متن کاملInfluence of pre-treatments on flexural strength of zirconia and debonding crack-initiation strength of veneered zirconia.
PURPOSE The aim of the present study was to assess the influence of pre-treatments of zirconia by sandblasting and/or heat treatment on the flexural strength of zirconia and debonding/crack-initiation strength of porcelain-veneered zirconia ceramic. MATERIALS AND METHODS Zirconia ceramic specimens were divided into four groups according to treatment (grinding as controls, sandblasting, heat t...
متن کاملInfluence of Veneering Fabrication Techniques and Gas-Phase Fluorination on Bond Strength between Zirconia and Veneering Ceramics.
PURPOSE Porcelain chipping has been one of the main problems of porcelain-fused-to-zirconia restorations. This study evaluates the bond strengths of layered, pressed, and adhesively bonded porcelain to yttria-stabilized zirconia substrates that have undergone traditional preparation or gas-phase fluorination. MATERIALS AND METHODS A three-point bending test was used to evaluate the bond stren...
متن کاملEffect of Glaze Cooling Rate on Mechanical Properties of Conventional and Pressed Porcelain on Zirconia.
The aim of this study was to characterize a conventional and a pressed porcelain for zirconia core as to biaxial flexural strength (BFS), apparent fracture toughness (FT) and microstructure composition, and to investigate the effect of glaze cooling rate on the BFS of the zirconia/porcelain bilayers. Monolayers of conventional porcelain Vita VM9 and pressed porcelain Vita PM9 (n=15) (12 mm diam...
متن کاملInfluence of surface modification techniques on shear bond strength between different zirconia cores and veneering ceramics
PURPOSE Veneering porcelain might be delaminated from underlying zirconia-based ceramics. The aim of this study was the evaluation of the effect of different surface treatments and type of zirconia (white or colored) on shear bond strength (SBS) of zirconia core and its veneering porcelain. MATERIALS AND METHODS Eighty zirconia disks (40 white and 40 colored; 10 mm in diameter and 4 mm thick)...
متن کامل