This study was designed to investigate the resistance to dislodgment provided by MTA HP, a new high-plasticity calcium silicate-based cement. Biodentine and White MTA Angelus were used as reference materials for comparison. Three discs 1 ± 0.1 mm thick were obtained from the middle third of the roots of 5 maxillary canines. Three 0.8-mm-wide holes were drilled on the axial surface of each root disc. Standardized irrigation was performed. Then the holes were dried with paper points and filled with one of the three tested cements. The filled dental slices were immersed in a phosphate-buffered saline (PBS) solution (pH 7.2) for 7 days before the push-out assessment. The Kruskal-Wallis test was applied to assess the effect of each endodontic cement on the push-out bond strength. Mann-Whitney with Bonferroni correction was used to isolate the differences. The alpha-type error was set at 0.05. All specimens had measurable push-out values and no premature failure occurred. There were significant differences among the materials (p <0.05). The Biodentine specimens had the highest push-out bond strength values (p < 0.05). MTA HP had significantly higher bond strength than White MTA (p < 0.05). MTA HP showed better push-out bond strength than its predecessor, White MTA; however, Biodentine had higher dislodgment resistance than both MTA formulations.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Blood Exposure on Push-Out Bond Strength of Four Calcium Silicate Based Cements

INTRODUCTION The purpose of this study was to compare the push-out bond strength of white ProRoot Mineral Trioxide Aggregate (MTA), Biodentine, calcium-enriched mixture (CEM) cement and Endosequence Root Repair Material (ERRM) putty after exposure to blood. METHODS AND MATERIALS A total of 96 root dentin slices with a standardized thickness of 1.00±0.05 mm and standardized canal spaces were r...

متن کامل

Apical adaptation, sealing ability and push-out bond strength of five root-end filling materials.

This study compared the fluid filtration, adaptation to the root canal walls, and the push-out bond strength of two resin-based sealers and three calcium silicate-based retrograde filling materials. Fifty maxillary canines were shaped using manual instruments and the apical portion was sectioned. Retrograde cavities of 3-mm depth were prepared. The specimens were divided into five groups (n = 1...

متن کامل

Push-out bond strength of intra-orifice barrier materials: Bulk- fill composite versus calcium silicate cement

Background. The aim of this study was to compare the push-out bond strengths of calcium silicate-based ProRoot MTA and Biodentine cements and SureFil SDR and EverX Posterior bulk-fill composite resins. Methods. Twenty-four single-rooted maxillary central incisors were sectioned below the cementoenamel junction, and the root canals were instrumented using rotary files. Thereafter, a parallel pos...

متن کامل

Physical evaluation of a new pulp capping material developed from portland cement

BACKGROUND This study examined the effects of addition of 10% and 25% by weight calcium hydroxide on the physicochemical properties of Portland cement associated with 20% bismuth oxide in order to develop a new pulp capping material. MATERIAL AND METHODS The solubility, pH value, setting time, compressive strength, and push out bond strength of modified Portland were evaluated and compared to...

متن کامل

Push-out bond strength of different mineral trioxide aggregates

OBJECTIVE This study was aimed to evaluate and to compare the push-out bond strength of different brands of mineral trioxide aggregate (MTA) with a calcium enriched mixture cement (CEM). MATERIALS AND METHODS Fifteen extracted, single-rooted human teeth were used. The middle-third of the roots were sliced perpendicular to the long axis into 1.00 ± 0.05 mm thick serial slices (15 root × 4 slic...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Brazilian oral research

دوره 30 1  شماره 

صفحات  -

تاریخ انتشار 2016