Impact of air-abrasion on fracture load and failure type of veneered anterior Y-TZP crowns before and after chewing simulation.

نویسندگان

  • Bogna Stawarczyk
  • Mutlu Ozcan
  • Lubica Hallmann
  • Malgorzata Roos
  • Albert Trottmann
  • Christoph H F Hämmerle
چکیده

The purpose of this study was to determine the fracture load and failure types of veneered zirconia crowns that were air-abraded on either the veneering or cementation surface. Fracture loads were determined before and after chewing simulation. Standardized Y-TZP frameworks (n = 360) for canines were fabricated and divided into one control group (n = 72) and 12 test groups (n = 24). The test groups were air-abraded using alumina powder (10 s, 2 bar, distance: 10 mm) with particle size of 50 μm resp. 110 μm and veneered with one of the veneering ceramics: Triceram, Zirox, or VITA VM9. The crowns were cemented on their corresponding CoCr abutment. The initial fracture load was measured in one half of each group (n = 12), and the other half (n = 12) was subjected to chewing cycling. The data were analyzed using three-way and one-way ANOVA, a post-hoc Scheffé test, two sample Student's t-test, and Weibull statistics (p < 0.05). Thus, nonaged, air-abraded groups of two veneering ceramics (Triceram, VITA VM9) showed higher mean fracture load compared to control groups. After chewing simulation, air-abraded groups showed lower mean fracture load compared to control groups. Aging decreased the Weibull modulus of all tested groups, and air-abraded groups showed lower Weibull moduli compared to control groups.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fracture of porcelain-veneered gold-alloy and zirconia molar crowns using a modified test set-up

Objective: The main aim of this study was to compare fracture load and fracture mode of yttria-stabilized tetragonal zirconia polycrystal (Y-TZP) and metal-ceramic (MC) molar crowns using a modified test set-up to produce fractures similar to those seen in vivo, i.e. fractures of the veneering material rather than complete fractures. Materials and methods: 13 high-noble-alloy MC and 13 Y-TZP mo...

متن کامل

Fracture Strength of Aged Monolithic and Bilayer Zirconia-Based Crowns

The purpose of this study was to evaluate the effect of design and surface finishing on fracture strength of yttria-tetragonal zirconia polycrystal (Y-TZP) crowns in monolithic (1.5 mm thickness) and bilayer (0.8 mm zirconia coping and 0.7 mm porcelain veneer) configuration after artificial aging. Bovine incisors received crown preparation and Y-TZP crowns were manufactured using CAD/CAM techni...

متن کامل

Influence of Different Framework Designs on the Fracture Properties of Ceria-Stabilized Tetragonal Zirconia/Alumina-Based All-Ceramic Crowns

The aim of this study was to evaluate the fracture load and failure mode of all-ceramic crowns with different ceria-stabilized tetragonal zirconia/alumina nanocomposite (Ce-TZP/A) framework designs. Four frameworks (anatomical shape: AS, with a buccal or lingual supporting structure: BS and LS, or buccal and lingual supporting structures: BLS) were fabricated. All frameworks were veneered with ...

متن کامل

Monolithic CAD/CAM lithium disilicate versus veneered Y-TZP crowns: comparison of failure modes and reliability after fatigue.

PURPOSE The aim of this research was to evaluate the fatigue behavior and reliability of monolithic computer-aided design/computer-assisted manufacture (CAD/CAM) lithium disilicate and hand-layer-veneered zirconia all-ceramic crowns. MATERIALS AND METHODS A CAD-based mandibular molar crown preparation, fabricated using rapid prototyping, served as the master die. Fully anatomically shaped mon...

متن کامل

Influence of cementation and cement type on the fracture load testing methodology of anterior crowns made of different materials.

To evaluate the influence of cementation on fracture load of anterior crowns made of CAD/CAM-resin-blocks (ART), leucite-reinforced glass-ceramics (LRG), lithium disilicate ceramics (LIT), veneered zirconia (ZRO) and veneered alloy (DEG). Each crown group (n=15/subgroup) was cemented on the metal abutment as follows: i. using glass ionomer, ii. using self-adhesive resin cement, and iii. not cem...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of biomedical materials research. Part B, Applied biomaterials

دوره 100 6  شماره 

صفحات  -

تاریخ انتشار 2012