Brittle fracture in associative polymers: the case of ionomer melts.

نویسندگان

  • Aamir Shabbir
  • Qian Huang
  • Quan Chen
  • Ralph H Colby
  • Nicolas J Alvarez
  • Ole Hassager
چکیده

Ionomers are interesting due to their applications in coatings, adhesives, films and packaging materials. A study of the underlying mechanisms for fracture in ionomers is consequently of both practical as well as theoretical interest. In this study, we employ high speed imaging coupled with uniaxial extensional rheometry to delineate the mechanics leading to the brittle fracture of ionomer melts. When these ionomers are elongated at a rate higher than the inverse relaxation time of physical crosslinks, an edge fracture occurs at a critical stress. Parabolic fracture profiles provide evidence that the phenomenon is purely elastic and bulk dissipation has little impact on the crack profile. Experimental results are interpreted within the Griffiths theory for linear elastic materials and the de Gennes theory for viscoelastic materials.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Dynamic and Quasi-Static Tensile Properties of Structural S400 Steel

The study of mechanical behavior of the structural steel S400 under quasi- static and dynamic loading has been the subject of this investigation. In oder to obtain different stress - triaxiality conditions the specimens were notched with 1, 1.5, 2 and 3.5 mm notch radius. The results of fractography show as the velocity of tension increases, ductility reduces and a ductile-brittle transition oc...

متن کامل

بررسی مقایسه‌ای خارج دهانی استفاده از سه نوع گلاس آینومر به عنوان لاینر چسبنده در افزایش مقاومت شکست دندانهای ترمیم شده با آمالگام

Statement of Problem: Because dental amalgam does not adhere to tooth structure, using adhesive cements in amalgam-bonded restorations have been increased. Purpose: The goal of this in-vitro study was to compare the effects of three types of glass ionomer as adhesive liners as well as varnish liner in increasing fracture resistance of teeth restored with amalgam. Materials and Methods: Seventy ...

متن کامل

A molecular dynamics simulation study of the influence of free surfaces on the morphology of self-associating polymers

Molecular dynamics simulations of thin films and bulk melts of model self-associating polymers have been performed in order to gain understanding of the influence of free surfaces on the morphology of these polymers. The self-associating polymers were represented by a simple bead-necklace model with attractive groups (stickers) at the chain ends (end-functionalized polymer) and in the chain int...

متن کامل

Multiple Cracks Propagate Simultaneously in Polymer Liquids in Tension.

Understanding the mechanism of fracture is essential for material and process design. While the initiation of fracture in brittle solids is generally associated with the preexistence of material imperfections, the mechanism for initiation of fracture in viscoelastic fluids, e.g., polymer melts and solutions, remains an open question. We use high speed imaging to visualize crack propagation in e...

متن کامل

HOT CRACK FORMATION IN PURE CU AND CU-30%ZN ALLOY DURING IN SITU SOLIDIFICATION

The hot cracking susceptibility can be determined by establishing the transition temperature between brittle and ductile fracture at high temperature tensile testing of in situ solidified samples. High temperature tensile properties were determined for commercial cathodic pure Cu and Cu- 30%Zn alloy. The transition temperatures for pure Cu and Cu-30%Zn were evaluated from ultimate tensile stres...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Soft matter

دوره 12 36  شماره 

صفحات  -

تاریخ انتشار 2016