Ž . The anodic polarization process in metal-hydride electrodes occurs via the following consecutive steps: i diffusion of absorbed Ž . hydrogen from the bulk to the surface of the electrode, ii hydrogen transfer from absorbed state to adsorbed state at the electrode Ž . surface, and iii electrochemical oxidation of the adsorbed hydrogen on the electrode surface. A theoretical treatment is presented to account for the dependencies on these three consecutive steps, of the reaction resistances, anodic limiting current, cathodic limiting current, and exchange current. The theoretical analysis predicts that the total resistances measured from linear micropolarization is the sum of the charge-transfer, hydrogen-transfer, and hydrogen-diffusion resistances, which is in contradiction with the generally accepted idea that the resistance measured from linear micropolarization is only the charge-transfer resistance. For a metal-hydride electrode with a Ž . flat pressure plateau at a low state of discharge SOD , the resistance measured from linear micropolarization is approximately equal to the sum of three resistances measured from AC impedance, namely, charge-transfer, hydrogen-transfer and hydrogen-diffusion resistances; however, when the SOD is high, the resistance measured from linear micropolarization is higher than total resistances measured from AC impedance. q 2000 Elsevier Science S.A. All rights reserved.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Eect of Co content on the kinetic properties of the MlNi4.3ÿXCoXAl0.7 hydride electrodes

By means of linear polarization, Tafel polarization and galvanostatic discharge methods, the kinetic properties of MlNi4.3ÿXCoXAl0.7 (X=0.0, 0.3, 0.5, 0.7, 0.9, 1.1 and 1.3) hydride electrodes, including high rate dischargeability HRD, exchange current density I0, limiting current density IL, the symmetry factor b, and the apparent di€usion coecient of hydrogen in the a phase Da have been stud...

متن کامل

Studies on the electrochemical properties of MlNi Co Al hydride 4 . 3 2 x x 0 . 7 alloy electrodes

In this paper, the electrochemical properties of MlNi Co Al electrode alloys, including high rate dischargeability, exchange 4.32x x 0.7 current density I , limiting current density I , and diffusion coefficient of hydrogen in the hydride D by means of linear polarization, 0 L a anodic polarization, and electrochemical impedance spectroscopy were systematically studied. The results indicate tha...

متن کامل

Metal hydrides for lithium-ion batteries.

Classical electrodes for Li-ion technology operate via an insertion/de-insertion process. Recently, conversion electrodes have shown the capability of greater capacity, but have so far suffered from a marked hysteresis in voltage between charge and discharge, leading to poor energy efficiency and voltages. Here, we present the electrochemical reactivity of MgH(2) with Li that constitutes the fi...

متن کامل

Evidence of the Potential Shift Mechanism in Crevice Corrosion (RESEARCH NOTES)

Previous research has indicated a qualitative resemblance between the current distribution along actively corroding crevice walls and currents measured in corresponding anodic polarization plots. Using detailed measurements of the potential gradient along the crevice, a semi-quantitative current distribution was calculated for the crevice wall using a double numerical differentiation method. Th...

متن کامل

Reaction Kinetics and X-Ray Absorption Spectroscopy Studies of Yttrium-Containing Metal Hydride Electrodes

This is a study of electrode degradation mechanisms and reaction kinetics of LaNi4.7Sn0.3, La(12x)YxNi4.7Sn0.3 (x 5 0.1, 0.2, and 0.3) and La0.7Y0.3Ni4.6Sn0.3Co0.1 metal hydride electrodes. Alloy characterization included X-ray diffraction, X-ray absorption (XAS), hydrogen absorption in a Sieverts apparatus, and electrochemical cycling of alloy electrodes. The atomic volume of H was determined ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2000