Haemocompatibility of Surface Modified AISI 316L Austenitic Stainless Steel Tested in Artificial Plasma

نویسنده

  • J. Przondziono
چکیده

The study comprises evaluation of suitability of passive layer created on the surface of AISI 316L stainless steel for products that are intended to have contact with blood. For that purpose, prior to and after chemical passivation, samples were subject to 7 day exposure in artificial plasma at the temperature of T=37°C. Next, tests of metallic ions infiltration from the surface to the solution were performed. The tests were performed with application of spectrometer JY 2000, by Yobin – Yvon, employing Inductively Coupled Plasma Atomic Emission Spectrometry (ICPAES). In order to characterize physical and chemical features of electrochemical processes taking place during exposure of samples to artificial plasma, tests with application of electrochemical impedance spectroscopy were suggested. The tests were performed with application of measuring unit equipped with potentiostat PGSTAT 302n with an attachment for impedance tests FRA2. Measurements were made in the environment simulating human blood at the temperature of T=37°C. Performed tests proved that application of chemical passivation process for AISI 316L stainless steel used for production of goods intended to have contact with blood is wellgrounded and useful in order to improve safety of their usage. Keywords—AISI 316L stainless steel, chemical passivation, artificial plasma, ions infiltration, EIS.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

An investigation on the passivation behavior of nitrogen enriched AISI 316L austenitic stainless steel

In the present work the effects of plasma nitridization on the passivation behavior of AISI 316L was investigated. To do this; nitriding treatments were carried out at 420°C for 1, 2, 4 and 16 hours. The phase composition and structure of the nitrided layer were studied by Low Angle X-ray diffraction and Scanning Electron Microscopy. The hardness of samples also was evaluated by Vickers microha...

متن کامل

Effect of plastic deformation on anelastic mechanical losses in multicomponent substitutional austenitic alloys

Complex two-component peak of anelastic mechanical losses was observed in multicomponent substitutional austenitic alloys after prior plastic deformation. In AISI 316L, AISI 316LN, AISI 310 and AISI 304 austenitic stainless steels, this peak is situated in the wide range of temperature from 200 to 400K. Characteristics of the observed peak for different thermo-mechanical treatments were studied...

متن کامل

Passivation and corrosion behaviours of AISI 316L stainless steel as implant materials in simulated blood environment

The purpose of the study was evaluation of corrosion resistance of steel 316L used in cardiologic treatment mainly for vascular stents. The study analysed influence of electrochemical and chemical treatment of the steel surface, including sterilisation with pressurised water steam, on its corrosion characteristics. The tests were performed in artificial blood plasma simulating human blood envir...

متن کامل

INFLUENCE OF SURFACE NANO/ULTRAFINE STRUCTURE ACHIEVED BY DEEP ROLLING PROCESS ON PLASMA NITRIDING AND TRIBOLOGICAL PROPERTIES OF THE AISI 316L STAINLESS STEEL

Influence of formation of surface nano/ultrafine structure using deep rolling on plasma nitriding and tribological properties of the AISI 316L stainless steel was investigated. Initially, the deep rolling process was carried out on the bar-shaped specimens at 15 cycles with 0.2 mm/s longitudinal rate and 22.4 rpm bar rotation. Then, plasma nitriding treatment was applied on the as-received...

متن کامل

Corrosion and microstructural analysis data for AISI 316L and AISI 347H stainless steels after exposure to a supercritical water environment.

This article presents corrosion data and microstructural analysis data of austenitic stainless steels AISI 316L and AISI 347H exposed to supercritical water (25 MPa, 550 °C) with 2000 ppb of dissolved oxygen. The corrosion tests lasted a total of 1200 h but were interrupted at 600 h to allow measurements to be made. The microstructural data have been collected in the grain interior and at grain...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2014