The Evolution of Cast Microstructures on the HAZ Liquation Cracking of Mar-M004 Weld

نویسندگان

  • Yi-Hsin Cheng
  • Jyun-Ting Chen
  • Ren-Kae Shiue
  • Leu-Wen Tsay
چکیده

The causes of liquation cracking in the heat-affected zone (HAZ) of a cast Mar-M004 superalloy weld were investigated. X-ray diffraction (XRD), electron probe microanalyzer (EPMA), and electron backscatter diffraction (EBSD) were applied to identify the final microconstituents at the solidification boundaries of the cast alloy. Fine borides and lamellar eutectics were present in front of some γ-γ′ colonies, which were expected to be liquefied prematurely during welding. The metal carbide (MC) enriched in Nb, Hf; M3B2 and M5B3 borides enriched in Cr and Mo; and lamellar Ni-Hf intermetallics were mainly responsible for the induced liquation cracking of the Mar-M004 weld, especially the MC carbides. Scanning electron microscope (SEM) fractographs showed that the fracture features of those liquation cracks were associated with the interdendritic constituents in the cast superalloy.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Analysis of Cracks in the Pulsed Nd:YAG Laser Welded Joint of Nickel-Based Superalloy

The weldability of GTD-111 nickel-based superalloy by pulsed Nd:YAG laser welding with an average power of 250 W was studied, and the microstructural evolution and cracking characteristics were also investigated. The solidification cracking of the fusion zone (FZ) and the intergranular liquation cracking in the heat affected zone (HAZ) were observed in the joint. Solidification cracking was cau...

متن کامل

Numerical Modeling of Heat Affected Zone Cracking Tendency during Laser and Hybrid Laser-Arc Welding Processes

A two-dimensional thermal elasto-plastic numerical model is developed by finite element method to analyze and compare the mechanical driving factor for heat affected zone (HAZ) liquation cracking during laser welding and hybrid laser-arc welding techniques. Calculations of transient temperatures and cooling rates are used in conjunction with solidification theory to analyze weld pool characteri...

متن کامل

Hot cracking in tungsten inert gas welding of magnesium alloy AZ91D

Plates of 3–5 mm in thickness were extracted from an AZ91D ingot and then butt joints of the plates were produced using tungsten inert gas (TIG) welding method. The TIG arc was also used to deposit welding beads on some of the thin plates. No cracking was found in the butt joints. However, hot cracking was always observed to propagate from the heat affected zone (HAZ) under the welding bead int...

متن کامل

EFFECT OF HEAT INPUT ON THE STRUCTURE AND PROPERTIES OF ALUMINIUM WELDMENT

The probable reasons for evolution of weld porosity and solidification cracking and the structure- property relationship in aluminium welds were investigated. Aluminium plates (1xxx series) were welded by Tungsten Inert Gas (TIG) welding process, 5356 filler metal was used and heat input was controlled by varying welding current (145A, 175A and 195A). The welded samples were examined under opti...

متن کامل

Transgranular liquation cracking of grains in the semi-solid state

Grain refinement via semi-solid deformation is desired to obtain superior mechanical properties of cast components. Using quantitative in situ synchrotron X-ray tomographic microscopy, we show an additional mechanism for the reduction of grain size, via liquation assisted transgranular cracking of semi-solid globular microstructures. Here we perform localized indentation of Al-15wt.%Cu globular...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2018