In the present work, novel Ultra-high molecular weight polyethylene (UHMWPE) composites reinforced with 3wt. %, 6wt. %, 9wt. %, 12wt. % and 15wt. % PEEK particles are fabricated by using hot compression moulding technique and mechanical properties are investigated. Experiments were conducted as per ASTM standards to evaluate the properties of tensile, flexural, impact, and microhardness. The results have revealed that the addition of PEEK to the UHMWPE reduced tensile strength and elongation at break, whereas the Young’s modulus of the composites was increased. The composite reinforced with 12 wt. % PEEK has better flexural properties and greater impact strength when compared to other composites. The hardness of the UHMWPE composites was increased based on PEEK content. The morphologies of the fractured surface are analyzed under field emission scanning electron microscope. The results have indicated poor interfacial bonding between PEEK and UHMWPE.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

In-Situ Polymerization of UHMWPE Using Bi-Supported Ziegler-Natta Catalyst of MoS2 Oxide/MgCl2 (Ethoxide Type)/TiCl4/TiBA: Study of Thermo-Mechanical Properties of System

The use of UHMWPE has attracted the attention of many researchers and industries. The aim of the present work is to fabricate UHMWPE/MoS2-Oxide nano-composites using in-situ polymerization. For this purpose, modified molybdenum disulfide was used. In order to perform the polymerization, a Ziegler-Natta catalytic system, with MoS2-Oxide and magnesium Ethoxide as support, was used. In order to fa...

متن کامل

Investigation of Wear Behavior of Biopolymers for Total Knee Replacements Through Invitro Experimentation

The average life span of knee prosthesis used in Total Knee Replacement (TKR) is approximately 10 to 15 years. Literature indicates that the reasons for implant failures include wear, infection, instability, and stiffness. However, the majority of failures are due to wear and tear of the prosthesis. The most common biopolymer used in TKR  is Ultra High Molecular Weight Polyethylene (UHMWPE). Pr...

متن کامل

Effect of Varying Silicon Carbide Particulate on the Mechanical Properties of Aluminium Based Alloy Automobile Brake Disc Component

In the current study, effect of varying Silicon Carbide particulate on the mechanical properties of Aluminium based alloy automobile brake disc component was investigated. The result of experimental investigation on mechanical properties of Silicon Carbide particle reinforced Aluminium Matrix was achieved for composite brake disc using universal tensile test machine, Rockwell hardness testing m...

متن کامل

Investigation of Mechanical Properties of Lithium-Based Geopolymer Composites Reinforced with Basalt Fibers

Recently, geopolymer binders have been considered because of low cost, simple processes for synthesis and many raw materials in nature. Geopolymer with brittle nature does not have high strength and cannot be used alone for structural materials. Therefore, to use in different structures, the composite which is reinforced with fibers such as carbon, glass, basalt, etchasbeen used. In this resear...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2016