This in vitro study investigated the aging behavior of dental composites with regard to surface roughness (SR), Vickers hardness (VH) and flexural strength (FS), and the study elucidated the impact of artificial aging parameters. One hundred and sixty-five rectangular specimens were prepared from five composites (Filtek Supreme XT, Filtek Silorane, CeramX, Quixfil, experimental ormocer) and subjected to various artificial aging protocols (storage in distilled water/ethanol/artificial saliva for 7, 90 and 365 days; thermal cycling, 2 x 3000 cycles 5/55 degrees C). SR, VH and FS were determined at baseline and after each aging treatment. Means and standard deviations were calculated; statistical analysis was performed using three-way ANOVA and the Tukey-Kramer multiple comparison test (alpha=.05). The results showed a significant influence in the composite and aging duration on mechanical parameters; the aging medium did not have a significant influence on VH and FS, but there was a significant influence on SR. The highest overall VH was found for theexperimental ormocer; Filtek Silorane yielded the lowest values. For FS, the significantly highest values were found for Filtek Silorane, and the lowest values were found for the experimental ormocer. Prolonged aging periods (90 or 365 days) or thermal cycling led to significant decreases in both VH and FS and significant increases in SR. The findings of the current study indicate that composites differ significantly for SR and its mechanical properties with regard to FS and VH, as well as in aging behavior. Generally, artificial aging leads to a significant decrease in mechanical properties, which underlines the relevance of continuous improvement of dental composites.
منابع مشابه
Influence of artificial aging on the shear bond strength of zirconia-composite interfaces after pretreatment with new 10-MDP adhesive systems
Introduction: This in-vitro study investigates the bond strength of different zirconia composites with three different modern adhesive systems after artificial aging using thermocycling and water storage. Methods: A total of 90 specimens of zirconia (InCoris, Sirona, Germany, Bernsheim) were ground using a 165 µm grit rotating diamond disc. Thirty specimens were additionally treated with eithe...
متن کاملThe Effect of Aging on Nano-Hardness and Modulus of Elasticity of Four Types of Composites: An in-vitro Study
Introduction: Resin composites are an important part of restorative treatment in modern dentistry. There are many trademarks available in Iran market and physico-chemical properties of many of these resin composites are not evaluated yet. This study was carried out to evaluate the physico-chemical properties of four available resin composites and also to assess the effect of aging on their prop...
متن کاملEnvironmental Effects on Mechanical Properties of Glass/Epoxy and Fiber Metal Laminates, Part I: Hygrothermal Aging
In this article, the effect of hygrothermal aging on mechanical properties of fiber metal laminates (FMLs) and E-glass/epoxy (GE) composites is investigated. First, FML and GE specimens were built using wet lay-up technique under vacuum pressure. Hygrothermal aging simulation was then carried out on both specimen types in distilled water at a constant temperature of 90 °C for 5 weeks. The resul...
متن کاملEnvironmental effects on mechanical properties of glass/epoxy and fiber metal laminates, Part II: Isothermal aging
The aim of this study is to investigate effects of isothermal aging on mechanical properties of fiber metal laminates (FMLs) and glass/epoxy composites. For this purpose, both materials were fabricated using the wet lay-up manufacturing technique under vacuum pressure. Both the glass/epoxy composites and the FML specimens were then subjected to isothermal aging (130°C, dried air) for up to 5 we...
متن کاملAccelerated Heat Aging Study of Phenolic/Basalt Fiber Reinforced Composites
One of the greatest impediments to use polymer-matrix composites is their susceptibility to degradation when exposed to the elevated temperatures and the limited knowledge on the thermal and mechanical properties of these composites at such temperatures. The objective of this study is to evaluate the effects of accelerated heat aging on the tensile properties of the Woven Basalt/Phenolic (WBP) ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Operative dentistry
دوره 35 4 شماره
صفحات -
تاریخ انتشار 2010