Improvement of the cleanability of pseudo-sensitized stainless steel surfaces by solution treatment.
نویسندگان
چکیده
Type 316L stainless steel particles were pseudo-sensitized by being heated at 700 degrees C for 100 h under a reduced pressure of 1.3 x 10(-3) Pa. Pseudo-sensitization treatment resulted in the formation of chromium-rich precipitates at the outermost surfaces of the stainless steel particles. The curve for the apparent surface charge density (sigma app) of the pseudo-sensitized particles showed a more basic character compared with the curve for the sigma app of the original particles. There was no significant difference between the amounts of bovine serum albumin (BSA) adsorbed on the original and the pseudo-sensitized particles. On the contrary, the efficiency of BSA removal from the pseudo-sensitized particles during batch-wise and continuous cleaning operations with 0.1M NaOH solution were significantly smaller than that for the original particles. It was indicated that the extremely lowered cleanability of the pseudo-sensitized particles was caused by a marked increase in the positive sigma app values after the pseudo-sensitization. Solution treatment of the pseudo-sensitized particles at 1,050 degrees C for 1 h under a reduced pressure of 1.3 x 10(-3) Pa could put again the chromium precipitates into a solid solution, thereby returning the surface chemical composition and the sigma app nearly to the original states. In addition, the solution-treated particles showed a good cleanability comparable to that of the original particles. These results demonstrated that solution treatment could improve the lowered cleanability of the pseudo-sensitized stainless steel surfaces.
منابع مشابه
DETERIORATION OF PITTING CORROSION OF 316 STAINLESS STEEL BY SENSITIZATION HEAT TREATMENT
In this research pitting Corrosion of a sensitized 316 stainless steel was investigated employing potentiodynamic, potentiostatic techniques. Sensitization process was carried out on as-received alloy by submitting the specimen in electric furnace set at 650°Cfor five hours and then the specimen was quenched 25°C water. Potentiodynamic polarization of as received and sensitized specimens in 1M ...
متن کاملAssessing the Cleanability of Stainless Steel Surfaces – Development of a Testing Method for Starch and Protein Based Soils
To measure the cleanability of stainless steel surfaces under standardized conditions, a test stand was set up. Three stainless steel plates (size 200 x 100 mm) can be fixed to the test stand and sprayed with a water jet from a low-pressure nozzle for a period of several minutes. The plates were previously soiled with a starch or protein film with a pre-defined layer thickness and dried for sev...
متن کاملFactors Affecting Weldability Improvement of Dissimilar Welds of Aged HP Stainless Steel and Alloy 800
The microstructure of HP stainless steel in aged and aged + solution annealed conditions and solutionized alloy 800 was characterized by optical microscopy, scanning electron microscopy (SEM), and transmission electron microscopy (TEM) equipped by EDS. All phases present in the above condition were described. The effects of solution annealing heat treatment temperature on the microstructure, te...
متن کاملStress Corrosion Cracking Detection of Sensitized Stainless Steel 304 in Chloride Media by Using Electrochemical Impedance Spectroscopy (EIS)
Electrochemical impedance spectroscopy (EIS) was used to detect stress corrosion cracking (SCC) in stainless steel 304 alloy exposed to an aqueous environment at 120 °C. Stainless steel 304 alloy as u-bend was tested in the solution that contains 40 weight percent of magnesium chloride. U-bended samples were prepared according to ASTM G30. EIS measurements were always performed simultaneously o...
متن کاملNanosecond Laser Surface Patterning of Bio Grade 316L Stainless Steel for Controlling its Wettability Characteristics
In this work, potential of the nanosecond laser processing technique on manipulating the surface wettability of 316L bio grade stainless steel is investigated. Results show that the steel wettability toward water, improves significantly after the laser treatment. Different analyses are assessed in correlation with wettability using Scanning Electron Microscope (SEM), Scanning Tunneling Microsco...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Biocontrol science
دوره 13 2 شماره
صفحات -
تاریخ انتشار 2008