Cu-doped p-type ZnO films are grown on c-sapphire substrates by plasma-assisted molecular beam epitaxy. Photoluminescence (PL) experiments reveal a shallow acceptor state at 0.15 eV above the valence band edge. Hall effect results indicate that a growth condition window is found for the formation of p-type ZnO thin films, and the best conductivity is achieved with a high hole concentration of 1.54 × 10(18) cm(-3), a low resistivity of 0.6 Ω cm, and a moderate mobility of 6.65 cm(2) V(-1) s(-1) at room temperature. Metal oxide semiconductor capacitor devices have been fabricated on the Cu-doped ZnO films, and the characteristics of capacitance-voltage measurements demonstrate that the Cu-doped ZnO thin films under proper growth conditions are p-type. Seebeck measurements on these Cu-doped ZnO samples lead to positive Seebeck coefficients and further confirm the p-type conductivity. Other measurements such as X-ray diffraction, X-ray photoelectron, Raman, and absorption spectroscopies are also performed to elucidate the structural and optical characteristics of the Cu-doped p-type ZnO films. The p-type conductivity is explained to originate from Cu substitution of Zn with a valency of +1 state. However, all p-type samples are converted to n-type over time, which is mostly due to the carrier compensation from extrinsic defects of ZnO.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Epitaxial Mn-doped ZnO diluted magnetic semiconductor thin films grown by plasma-assisted molecular-beam epitaxy

A growthwindow for theMn effusion cell temperature (TMn) is demonstrated for epitaxialMn-doped ZnO (MnZnO) thin films grown on sapphire substrates using molecular-beam epitaxy. Within the growth window, the films are ferromagnetic with the largest saturated magnetization occurring at TMn1⁄4700 1C. The Curie temperature of these MnZnO diluted magnetic semiconductor thin films is above roomtemper...

متن کامل

Correlation between crystal structure and optical properties of copper- doped ZnO thin films

ZnO and Cu doped[1] (CZO) thin films were prepared by radio frequency sputtering. The structural and optical properties of thin films were investigated using X-ray diffraction (XRD), atomic force microscopy (AFM), optical spectrophotometer, and photoluminescence (PL) techniques. ZnO thin films showed crystalline and micro-stress defects in the crystal lattice. Annealing of CZO thin films increa...

متن کامل

Atmospheric oxygen in Mn doped GaAs/GaAs(0 0 1) thin films grown by molecular beam epitaxy

Mn doped GaAs thin films were grown using molecular beam epitaxy at high and low substrate temperatures. The elemental concentration depth profiles in the thin films were determined by using Auger electron spectroscopy combined with ion etching. The Mn concentration is higher near the surface and then decreases with depth for films grown at high substrate temperatures. The Mn concentration prof...

متن کامل

Study of the effect of plasma power on ZnO thin films growth using electron cyclotron resonance plasma-assisted molecular-beam epitaxy

ZnO thin films were grown on r-plane sapphire substrates using electron cyclotron resonance (ECR) plasma-assistedmolecular-beam epitaxy. The effect of the oxygen ECR plasma power on the growth rate, structural, electrical, and optical properties of the ZnO thin films were studied. It was found that larger ECR power leads to higher growth rate, better crystallinity, lower electron carrier concen...

متن کامل

Ga-related photoluminescence lines in Ga-doped ZnO grown by plasma-assisted molecular-beam epitaxy

Low-temperature photoluminescence PL and temperature-dependent Hall-effect T-Hall measurements were carried out in undoped and Ga-doped ZnO thin films grown by molecular-beam epitaxy. As the carrier concentration increases from 1.8 1018 to 1.8 1020 cm−3, the dominant PL line at 9 K changes from I1 3.368–3.371 eV to IDA 3.317–3.321 eV , and finally to I8 3.359 eV . The dominance of I1, due to io...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • ACS applied materials & interfaces

دوره 7 16  شماره 

صفحات  -

تاریخ انتشار 2015