Characterization of Tungsten Inert Gas (TIG) Welding Fume Generated by Apprentice Welders
نویسندگان
چکیده
Tungsten inert gas welding (TIG) represents one of the most widely used metal joining processes in industry. Its propensity to generate a greater portion of welding fume particles at the nanoscale poses a potential occupational health hazard for workers. However, current literature lacks comprehensive characterization of TIG welding fume particles. Even less is known about welding fumes generated by welding apprentices with little experience in welding. We characterized TIG welding fume generated by apprentice welders (N = 20) in a ventilated exposure cabin. Exposure assessment was conducted for each apprentice welder at the breathing zone (BZ) inside of the welding helmet and at a near-field (NF) location, 60cm away from the welding task. We characterized particulate matter (PM4), particle number concentration and particle size, particle morphology, chemical composition, reactive oxygen species (ROS) production potential, and gaseous components. The mean particle number concentration at the BZ was 1.69E+06 particles cm(-3), with a mean geometric mean diameter of 45nm. On average across all subjects, 92% of the particle counts at the BZ were below 100nm. We observed elevated concentrations of tungsten, which was most likely due to electrode consumption. Mean ROS production potential of TIG welding fumes at the BZ exceeded average concentrations previously found in traffic-polluted air. Furthermore, ROS production potential was significantly higher for apprentices that burned their metal during their welding task. We recommend that future exposure assessments take into consideration welding performance as a potential exposure modifier for apprentice welders or welders with minimal training.
منابع مشابه
Exposure to Inhalable, Respirable, and Ultrafine Particles in Welding Fume
This investigation aims to explore determinants of exposure to particle size-specific welding fume. Area sampling of ultrafine particles (UFP) was performed at 33 worksites in parallel with the collection of respirable particles. Personal sampling of respirable and inhalable particles was carried out in the breathing zone of 241 welders. Median mass concentrations were 2.48 mg m(-3) for inhalab...
متن کاملWelding of 304L Stainless Steel with Activated Tungsten Inert Gas Process (A-TIG)
Gas tungsten arc welding is a popular process in those applications requiring a high degree of quality and accuracy. However, this process has a big disadvantage against the substantially high productivity welding procedures. Hence, many efforts have been made to improve its productivity. One of these efforts is the use of activating flux (A-TIG welding). In this study, the performance of A-TIG...
متن کاملThorium-232 exposure during tungsten inert gas arc welding and electrode sharpening.
To assess the exposure of welders to thorium-232 (232Th) during tungsten inert gas arc (TIG) welding, airborne concentrations of 232Th in the breathing zone of the welder and background levels were measured. The radioactive concentrations were 1.11 x 10(-2) Bq/m3 during TIG welding of aluminum (TIG/Al), 1.78 x 10(-4) Bq/m3 during TIG welding of stainless steel (TIG/SS), and 1.93 x 10(-1) Bq/m3 ...
متن کاملPersonal Exposure among Welders and Non-welders
The objective of this study was to characterize personal exposures to welding-related metals and gases for production welders and non-welders in a large manufacturing facility. Welding fume metals and irritant gases nitrogen dioxide (NO2) and ozone (O3) were sampled for thirty-eight workers. Personal exposure air samples for welding fume metals were collected on 37 mm open face cassettes and ni...
متن کاملStructure-property Interaction in Flux Assisted Tungsten Inert Gas Welding of Austenitic Stainless Steel
Austenitic stainless steel SS304 grade was welded with active Tungsten Inert Gas (TIG) welding process by applying a flux paste made of SiO2 powder and acetone. SiO2 flux application improves the weld bead depth with a simultaneous reduction in weld bead width. The improvement in penetration results from arc constriction and reversal of Marangoni convection. Experimental studies revealed that t...
متن کامل