Evaluation of Fatigue Damage in Adhesive Bonding: Part 1: Bulk adhesive

نویسندگان

  • M. M. Abdel Wahab
  • Magd Abdel Wahab
چکیده

The measurement of damage constants in adhesive bonding has been investigated. Bulk adhesive was used in this study for two reasons: a) stress distribution in bulk adhesive is simpler than adhesive in joints and b) specimen dimensions met fatigue test standard. Bulk adhesive was made from film-form of epoxy resin. In general, the characteristics and the behaviour of bulk adhesive may differ from adhesive in joint because of the presence of voids and the constrains imposed by the substrates. Low cycle fatigue tests with load amplitude ratio of 0.1 at frequency 5 Hz were performed to determine the damage variable as a function of number of cycles. Damage curves, i.e. evolution of damage variable as a function of number of cycles, were derived and plotted using isotropic damage equation. Damage was evaluated using the decrease of stress range during lifecycles of a constant displacement amplitude test. It was found that damage curves were fitted well by low cycle fatigue damage evolution law equation. This equation was derived from a dissipation potential function. Curve fitting was performed using Robust Least Square rather than ordinary linear least square because damage curves have extreme points (usually near failure point). It was found that fitting process could not converge for adhesive fracture at higher cycles (Nf > 9000). Two damage constants A

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Evaluation of Fatigue Damage in Adhesive Bonding: Part 2: Single lap joint

Damage parameters for crack initiation in Single Lap Joint (SLJ) are determined by combining continuum damage mechanics, Finite Element Analysis (FEA) and fatigue experimental data. Even tough SLJ has a simple configuration; the stresses in the adhesive region are quite complex and exhibit a multi-axial state. Such a condition leads to the need to introduce a general value of triaxiality functi...

متن کامل

Microleakage under Orthodontic Metal Brackets Bonded with Three Different Bonding Techniques with/without Thermocycling

Introduction: The aim of this study was to compare the microleakage of beneath the orthodontic brackets bonded with 3 different bonding techniques and evaluate the effect of thermocycling. Methods: One hundred and twenty premolars were randomly divided into 6 groups, received the following treatment: group 1: 37% phosphoric acid gel+Unite primer+Unite adhesive, group 2: 37% phosphoric acid gel+...

متن کامل

Fatigue Crack Growth in Adhesive Joints

Adhesive joining is recognized as a potential enabling technology for a variety of material systems being considered in automotive structures where traditional fastening methods would be inappropriate. Well known examples include fiber reinforced composites and polymers. Additionally in certain circumstances, adhesive bonding of steel structures can provide benefits such as improved stiffness a...

متن کامل

Evaluation of the effect of two different desensitizing agents on shear bond strength of universal adhesive resin (an invitro study )

Background and Aim: dentin desensitizers may affect dentin organic matrix properties or occlude dentinal tubules which may have adverse effects on the bonding performance of adhesive systems. The aim of this study was invitro evaluation of Gluma desensitizer and Tokuyama Shield Plus effects or shear bond strength of (BISCO) all-bond universal bonding  system. Materials and Methods: 30 caries f...

متن کامل

Comparative evaluation of microleakage of composite restorations using fifth and seventh generations of adhesive systems

Introduction: Simultaneous etching of enamel and dentin using the novel generation of adhesive systems with contracted operational steps, has shown a good clinical efficacy. The aim of this study was to evaluate the microleakage of composite restorations using the V and VII generations of adhesive systems on primary teeth. Methods: This study was performed on 45 human intact extracted primar...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2009