Evaluation of metal and carbon monoxide exposures during steel slab cutting and slitting.
نویسندگان
چکیده
This Health Hazard Evaluation (HHE) report and any recommendations made herein are for the specific facility evaluated and may not be universally applicable. Any recommendations made are not to be considered as final statements of NIOSH policy or of any agency or individual involved. Additional HHE reports are available at The employer shall post a copy of this report for a period of 30 calendar days at or near the workplace(s) of affected employees. The employer shall take steps to insure that the posted determinations are not altered, defaced, or covered by other material during such period.
منابع مشابه
Solidification and thermal performance analysis of the low carbon steel during the continuous casting process
The present paper evaluates the effect of the nozzle characteristics on the heat transfer and phase change of the low carbon steel during the continuous casting process. A three-dimensional energy equation and a solidification model are used to drive the governing equation of the phase change and temperature distribution. A linear relation is obtained to predict the temperature-dependent of the...
متن کاملEvaluation of dissimilar joint properties of A321 austenitic stainless steel to A537CL1 carbon steel by GTAW process
In this research, the microstructure and mechanical behavior of dissimilar joint of AISI 321 stainless steel to ASTM A57CL1 were studied. For this purpose, the GTAW process and ER 308L filler metal with diameter of 1.8 mm were used. In order to study the microstructure and fracture surface of weld samples, optical microscope and scanning electron microscope (SEM) were used. Also, the mechanical...
متن کاملEvaluation of dissimilar joint properties of A321 austenitic stainless steel to A537CL1 carbon steel by GTAW process
In this research, the microstructure and mechanical behavior of dissimilar joint of AISI 321 stainless steel to ASTM A57CL1 were studied. For this purpose, the GTAW process and ER 308L filler metal with diameter of 1.8 mm were used. In order to study the microstructure and fracture surface of weld samples, optical microscope and scanning electron microscope (SEM) were used. Also, the mechanical...
متن کاملEvaluation of the Melted Zone Microstructure in the Interface of the Dissimilar Weld between A335 Low Alloy Steel and ER309L Filler Metal by Gas Tungsten Arc Welding
In the present study, the microstructure and mechanical properties of the dissimilar welding between ASTM A335 low alloy steel and ER309L austenitic stainless steel were investigated using the gas tungsten arc welding process. The welding of dissimilar materials between ASTM A335 low alloy steel and ER309L austenitic stainless steel was found to have a significant effect on the microstructure w...
متن کاملOccupational exposure to dioxins by thermal oxygen cutting, welding, and soldering of metals.
This paper focuses on one aspect of occupational dioxin exposure that is novel and unexpected. Exposures in excess of the German threshold limit value of 50 pg international toxicity equivalent (I-TEQ)/m3 are very frequent, unpredictable, and sometimes very high--up to 6612 pg I-TEQ/m3--during thermal oxygen cutting at scrap metal and demolition sites. The same procedure involving virgin steel ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Journal of occupational and environmental hygiene
دوره 10 5 شماره
صفحات -
تاریخ انتشار 2013