Shear Bond Strengths of Different Adhesive Systems to Biodentine

نویسندگان

  • Mesut Enes Odabaş
  • Mehmet Bani
  • Resmiye Ebru Tirali
چکیده

The aim of this study was to measure the shear bond strength of different adhesive systems to Biodentine with different time intervals. Eighty specimens of Biodentine were prepared and divided into 8 groups. After 12 minutes, 40 samples were randomly selected and divided into 4 groups of 10 each: group 1: (etch-and-rinse adhesive system) Prime & Bond NT; group 2: (2-step self-etch adhesive system) Clearfil SE Bond; group 3: (1-step self-etch adhesive systems) Clearfil S(3) Bond; group 4: control (no adhesive). After the application of adhesive systems, composite resin was applied over Biodentine. This procedure was repeated 24 hours after mixing additional 40 samples, respectively. Shear bond strengths were measured using a universal testing machine, and the data were subjected to 1-way analysis of variance and Scheffé post hoc test. No significant differences were found between all of the adhesive groups at the same time intervals (12 minutes and 24 hours) (P > .05). Among the two time intervals, the lowest value was obtained for group 1 (etch-and-rinse adhesive) at a 12-minute period, and the highest was obtained for group 2 (two-step self-etch adhesive) at a 24-hour period. The placement of composite resin used with self-etch adhesive systems over Biodentine showed better shear bond strength.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of salivary contamination on shear bond strength of three different dentin adhesive systems

Effect of salivary contamination on shear bond strength of three different dentin adhesive systems Dr. H. Kermanshah* - Dr. H. Haj miragha** - Dr. SH. Gatoeizadeh*** *- Assistant Professor of Operative Dentistry Dept. - Faculty of Dentistry – Tehran University / Medical Sciences. **- Assistant Professor of Fixed Prosthodontics Dept. & Dental Research Center - Faculty of Dentistry – Tehran Unive...

متن کامل

Evaluation of Shear Bond Strengths of Three Adhesive Materials Used to Retain Fiber Post in the Severely Damaged Primary Anterior Teeth

Background and Objective: Tooth decay and periodontal problems are among the most common human diseases which are considered unsolved health problems in most countries of the world. This study aimed to investigate and compare the shear bond strength of the fiber post with three different types of cement, including Glass ionomer, as well as Universal and Flowable composites. Materials and Metho...

متن کامل

Shear bond strength of Biodentine, ProRoot MTA, glass ionomer cement and composite resin on human dentine ex vivo

INTRODUCTION The aim of this study was to compare the shear bond strength of Biodentine, ProRoot MTA (MTA), glass ionomer cement (GIC) and composite resin (CR) on dentine. METHODS 120 extracted human third molars were embedded in cold-cured-resin and grinned down to the dentine. For each material 30 specimens were produced in standardised height and width and the materials were applied accord...

متن کامل

Comparison of Shear Bond Strength of Composite Restorations to Intact Enamel of Primary Incisors When Using Different Conditioners and Adhesive Systems

Introdouction: Esthetic demands of patients have led to the introduction of tooth-colored restorations wherecomposite resins are bonded to the enamel using acid etch techniques. Total etch adhesion systems are still considered as the gold standard among bonding systems. However, clinicians have a tendency to use adhesive systems with simpler application procedures. The aim of the present stu...

متن کامل

استحکام باند برشی آمالگام به عاج با استفاده از سیستم‌های چسبنده عاجی

Background and Aims: The aim of this in vitro study was to assess the shear bond strength of amalgam to dentin using four dentin adhesive systems.Materials and Methods: One hundred human molars were selected. After enamel removal, a dentin cylinder with 3 mm thickness was prepared. Eighty specimens were resorted with amalgam and four dentin adhesive systems as follows (n=20): group 1, Scotch Bo...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 2013  شماره 

صفحات  -

تاریخ انتشار 2013