Fracture strength of ceramic bracket tie wings subjected to tension.

نویسندگان

  • Gerald Johnson
  • Mary P Walker
  • Katherine Kula
چکیده

One of the most common areas of ceramic bracket fracture is within the tie-wing complex. When an archwire is ligated into position, tensile forces are placed under the tie wing. However, no study, to date, has focused specifically on the fracture resistance of the tie-wing complex. The aim of this study is to compare the tensile fracture strength of seven currently available ceramic brackets (Inspire, Fascination, Mystique, InVu, Clarity, Virage, and Luxi) as a function of bracket brand and bracket configuration, semitwin vs true-twin. Based on a power analysis of pilot data, 10 maxillary central incisor brackets per group were tested to failure with a tensile load placed directly under the distoincisal tie wing. The results ranged from a maximum mean fracture strength of 147.71 (5.87) MPa with Fascination brackets to a minimum mean fracture strength of 84.28 (7.01) MPa with Luxi brackets. The statistical analysis indicated a significant effect on fracture strength as a function of bracket brand (P < .05) and that semitwin brackets, Fascination, Mystique, and Virage, had significantly higher fracture strength than true-twin brackets, Clarity, lnVu, and Luxi (P < .05). Interestingly, the only monocrystalline bracket in the study, Inspire, could not be fractured using the investigation protocol. In fact, the steel ligature fixture wire would break before tie-wing fracture at a mean fixture failure of 198.65 MPa.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

In vitro orthodontic bracket bonding to porcelain.

This in vitro study investigated the influence of using different combinations of bracket, adhesive, and light-curing source on the tensile bond strength to porcelain and on failure patterns at debonding. Tensile tests were performed using: one ceramic bracket versus one metal bracket, two orthodontic composites; type bisphenol A-glycidyldimethacrylate and urethane dimethacrylate (UDMA), and fo...

متن کامل

Evaluation of the bond strength of different bracket-bonding systems to bovine enamel.

In an experimental study the bond strength of stainless steel, ceramic and plastic brackets to bovine enamel was investigated by tensile testing. The brackets were cemented to the enamel using a conventional two-paste orthodontic bonding resin, a light-cured, fluoride-releasing adhesive, a no-mix-orthodontic bonding resin and a light-curing glass ionomer cement. For evaluation of the experiment...

متن کامل

Influence of surface conditioning on ceramic microstructure and bracket adhesion.

The objective of this study was to investigate the influence of different conditioning procedures on various ceramic microstructures and bracket adhesion. Ceramic specimens (feldspathic, leucite, leucite-free, and fluorapatite) were mechanically conditioned (n = 20 per ceramic type) with conventional hydrofluoric acid (5 per cent HF; 60/30 seconds), buffered hydrofluoric acid (9.6 per cent BHF;...

متن کامل

Effect of self-etching primer/adhesive and conventional bonding on the shear bond strength in metallic and ceramic brackets

INTRODUCTION Bracket debonding from the tooth surface is a common problem in fixed orthodontics. The aims of the present study were to assess the bond strength and failure sites in two ways of bonding technique, with metallic and ceramic brackets. MATERIALS AND METHODS One hundred premolars were assigned to 4 groups of 25 each: Group A, metallic brackets/conventional procedure; Group B, metal...

متن کامل

The in-vitro clinical failure of all-ceramic crowns and the connector area of fixed partial dentures: the influence of interfacial surface roughness.

OBJECTIVES To assess the effect of interfacial surface roughness on the flexure strength and fracture mode and origin utilizing an in-vitro assessment of the clinical failure conditions expected for all-ceramic crowns and the connector area of fixed partial dentures (FPDs) using bilayered ceramic specimens tested in bi-axial flexure. METHODS Sets of 20 bilayered composite discs, with core:den...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • The Angle orthodontist

دوره 75 1  شماره 

صفحات  -

تاریخ انتشار 2005