Reduced UHMWPE Wear Using Magnesia-Stabilized Zirconia Femoral Components in High Kinematics/High Load Knee Simulator Tests

ثبت نشده
چکیده

188 ©2013 Society For Biomaterials

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Polyethylene Wear Debris From a Knee Simulator Model: Effect of Crosslinking and Counterface Material

INTRODUCION: Improved wear resistance of crosslinked UHMWPE has been well demonstrated in both hip and knee [1-4]. A reduction of 70% can be shown in knee simulators from conventional crosslinked tibial inserts (CXPE) gamma-irradiated at 3.5Mrad to 7Mrad highly crosslinked inserts (HXPE). Hip simulator models indicated that debris size decreased with increased crosslinking [5]. In the knee it h...

متن کامل

Using a surrogate contact pair to evaluate polyethylene wear in prosthetic knee joints.

With recent improvements to the properties of ultra-high molecular weight polyethylene (UHMWPE) used in joint replacements, prosthetic knee and hip longevity may extend beyond two decades. However, it is difficult and costly to replicate such a long in vivo lifetime using clinically relevant in vitro wear testing approaches such as walking gait joint simulators. We advance a wear test intermedi...

متن کامل

Investigation of Wear Behavior of Biopolymers for Total Knee Replacements Through Invitro Experimentation

The average life span of knee prosthesis used in Total Knee Replacement (TKR) is approximately 10 to 15 years. Literature indicates that the reasons for implant failures include wear, infection, instability, and stiffness. However, the majority of failures are due to wear and tear of the prosthesis. The most common biopolymer used in TKR  is Ultra High Molecular Weight Polyethylene (UHMWPE). Pr...

متن کامل

Mobile or fixed unicompartmental knee prostheses? In-vitro wear assessments to solve this dilemma.

The unicompartmental knee prosthesis is an attractive alternative to total knee arthroplasty. Current UKP devices can be subdivided into two groups based on different design principles: fixed bearing knees, where the ultra-high molecular weight polyethylene meniscal component snap or press fits into the tibial tray, and mobile bearing designs which facilitate movement of the insert relative to ...

متن کامل

A Low Conforming, Low Wear Solution in Fixed Bearing Total Knee Prostheses

Introduction: Ultra High Molecular Weight Polyethylene (PE) remains the primary bearing surface of choice in total knee replacements (TKR). Traditionally Archard’s Law is used to predict wear rates in hip and knee prostheses. This assumes that the volume of wear between two articulating surfaces is proportional to the applied load and sliding distance. However it has been shown that this is a s...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2013