The force levels required to mechanically debond ceramic brackets: an in vitro comparative study.

نویسندگان

  • S Arici
  • C Minors
چکیده

The in vitro force levels generated by four differing methods of mechanical debonding techniques for ceramic brackets, using debonding pliers, were measured. The forces generated using wide (method W) and narrow blades (method N) were compared with those generated using a diagonally opposite corner application of the wide blades (method C) and incisal-gingival application of a pair of pointed blades (method P). Chemically retained ceramic brackets (Transcend) were bonded to bovine teeth using a filled, two-paste, chemically cured composite (Concise). After 24 hours storage at 37 degrees C in water, each specimen was subjected to one of the four mechanical debonding methods in a custom-built jig, simulating the clinical application of conventional debonding pliers. A one-way ANOVA with a Tukey's honestly significant difference test revealed statistically significant differences in debonding strengths between the four methods at the 0.05 level of significance. The mean debonding strength generated by method C was 40 and 25 per cent lower than that for methods W and N, respectively. Scoring of the adhesive remnant index (ARI) revealed that the predominant bond failure site was at the bracket/adhesive interface for all groups. Macroscopically, no enamel damage or bracket fractures were observed.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Force to debond brackets from high-fusing and low-fusing porcelain systems.

The purpose of this study was to test the hypothesis that porcelain surface finishing, ie, low- and high-fusing porcelain, has an effect on the amount of force required to debond orthodontic brackets. A total of 20 high-fusing and 20 low-fusing porcelain specimens were prepared, polished, and bonded with standard edgewise brackets using a suggested porcelain bonding protocol. The brackets were ...

متن کامل

Shear Bond Strength of Orthodontic Brackets Bonded to Zirconium Crowns

BACKGROUND An increasing demand for esthetic restorations has resulted in an increased use of all-ceramic restorations, such as zirconium. However, one of the challenges the orthodontist must be willing to face is how to increase bond strength between the brackets and various ceramic restorations.Bond strength can beaffected bybracket type, by the material that bracketsaremade of, and their bas...

متن کامل

Comparative Evaluation of Friction Resistance of Titanium, Stainless Steel, Ceramic and Ceramic with Metal Insert Brackets with Varying Dimensions of Stainless Steel Wire: An In vitro Multi-center Study

BACKGROUND The orthodontist seeks an archwire-bracket combination that has both good biocompatibility and low friction. Hence, the aim of this multicenter in vitro study was to evaluate and compare the frictional resistance generated between titanium (Ti), stainless steel (SS), ceramic and ceramic with metal insert (CMI) brackets with SS wires of varying dimensions in a specially designed appar...

متن کامل

Effect of CO2 laser irradiation on the surface of the polycrystalline ceramic bracket and the rate of canine movement with sliding mechanic

Introduction: Metal brackets are the most commonly used brackets in clinical orthodontics, but the sight of color of the metal bracket can be unpleasant for some patients. Ceramic brackets offer the desired beauty but they have higher frictional resistance.  Considering that in vitro studies suggest that CO2 laser reduces the friction between the wire and slot of the bracket in the sliding mech...

متن کامل

Comparative Evaluation of Frictional forces between different Archwire-bracket Combinations

Introduction: During sliding mechanics, frictional resistance is an important counterforce to orthodontic tooth movement; which must be controlled to allow application of light continuous forces. objective: To investigate static and kinetic frictional resistance between three orthodontic brackets: ceramic, self-ligating, and stainless steel, and three 0.019×0.025” archwires: stainless steel, ni...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • European journal of orthodontics

دوره 22 3  شماره 

صفحات  -

تاریخ انتشار 2000