Pii: S1359-6454(99)00140-8
نویسندگان
چکیده
ÐAn electrophoretic deposition (EPD) technique is used to prepare porous alumina membranes. The deposition kinetics which are conventionally derived based on a mass conservation law have been modi®ed in terms of the thickness of the deposited layer. This modi®cation allows the porosity evolution of the membrane to be predicted under a variety of EPD processes. A transition in deposition from linear to parabolic kinetics is observed which has been further veri®ed by a subsequent microstructure examination. The deposited layers are increasingly uniform and dense in structure with increasing deposition time over the parabolic kinetic regime; whilst a more porous packing is observed during the initial deposition time period, corresponding to the linear kinetic regime. The microstructural evolution of the EPD membranes appears to agree well with the porosity equations derived based on an analytical combination of both experimentally-derived formula and the corresponding kinetic model. # 1999 Acta Metallurgica Inc. Published by Elsevier Science Ltd. All rights reserved.
منابع مشابه
Pii: S1359-6454(99)00264-5
ÐThe grain boundary segregation of Bi in dilute polycrystalline Cu±Bi alloys was systematically studied as a function of temperature and composition. The temperature dependencies of the Gibbsian excess of Bi at the grain boundaries exhibited discontinuous changes at the temperatures close to, but dierent from the bulk solidus temperatures. The observed segregational phase transition was interp...
متن کاملPii: S1359-6454(99)00156-1
ÐThe eect of hydrogen in solid solution on the edge/screw character of dislocations has been investigated by deforming samples of high-purity aluminum in a gaseous hydrogen environment in situ in a controlled environment transmission electron microscope. Solute hydrogen was found to stabilize edge segments of dislocations, which inhibited, and in some cases stopped dislocations from cross-slip...
متن کاملPii: S1359-6454(99)00023-3
ÐThe durability of residually compressed coatings, particularly thermal barrier coatings (TBCs), is governed by events occurring at the interface with the substrate. In general, failure involves the sequential nucleation growth and coalescence of separations in the presence of imperfections and defects. The growth and coalescence phases are analyzed. Remnant ligaments are expected from the mech...
متن کاملPii: S1359-6454(99)00280-3
ÐOngoing research is reported aimed at improving bio®xation through the use of bioactive glass coatings on Ti-based implant alloys. The optimized processing conditions for coating with one promising bioactive glass composition are discussed, and the stress corrosion crack growth behavior in a simulated human physiological environment is presented. This glass can be successfully used to coat Ti ...
متن کاملPii: S1359-6454(96)00395-3
Debonding of films attached to substrates as well as fibers embedded in matrices typically involves initiation, steady-state propagation and a final transient as the debond converges on an edge or another debond. The emphasis in this paper is on the mechanics of the transient. Under most circumstances, a converging debond crack is characterized by an energy release rate that approaches zero, ca...
متن کامل