Examining the Pearlite Growth Interface in a Fe-C-Mn Alloy
نویسندگان
چکیده
A method of collecting composition data and examining structural features of pearlite lamellae and the parent austenite at the growth interface in a 13wt. % manganese steel has been demonstrated with the use of Scanning Transmission Electron Microscopy (STEM). The combination of composition data and the structural features observed at the growth interface show that available theories of pearlite growth cannot explain all the observations. Keywords—Interfaces, Phase transformations, Pearlite, Scanning Transmission Electron Microscopy (STEM).
منابع مشابه
The Non-Steady State Growth of Pearlite outside the Hultgren Extrapolation
The goal of this paper is to analyse the effect of adding Al on the non-steady pearlite growth occurring in a Fe-C-Mn system. The results are discussed in terms of the partitioning of elements across the austenite/ferrite and austenite/cementite interfaces, and the modification of the pearlite driving force related to the change in carbon activity in austenite.
متن کاملEffects of Carbon Content and Cold Working on Damping Capacity and Mechanical Property of Fe-17wt.%Mn Martensitic Alloy
Effect of carbon content on damping capacity of Fe-l7%Mn alloy is investigated by varying the carbon content from 0.02wt% to 0.28wt%. And cold rolling is conducted to examine its influence on damping capacity and mechanical properties in an Fe-17%Mn-0.02%C alloy. With the increase in carbon content, damping capacity decreases due to the area reduction of 7 / E boundaries and their mobility. Col...
متن کاملThe effect of carbon distribution on the manganese magnetic moment in bcc Fe-Mn alloy.
First-principles calculations were performed to study the structural, electronic, and magnetic properties of bcc Fe with C impurities alloyed with 2, 3, and 6 at.% of Mn. Our results reveal that both manganese concentration and carbon location with respect to Mn affect the Fe-Mn magnetic interaction. With an increase in Mn concentration in bcc Fe-Mn alloy, the local magnetic moment of manganese...
متن کاملEffect of surface-applied reactive elements on the early stage oxidation of Fe- 18Cr-5Al and Fe-18Cr-5Al-1Hf alloys
The effect of lanthanum implantation on the early stage oxidation of Fe-18wt%Cr5wt%Al and Fe-l8wt%Cr-5wt%Al-Iwt%Hf alloys at 1100 OC has been investigated. I t was found that the reactive element enriched surfaces oxidized almost two times faster initially, and the scale that formed had a higher iron content. An extremely wavy scale/alloy interface developed in the early stage due to the accele...
متن کاملTransformation Behavior and its Effect on Damping Capacity in Fe-Mn Based Alloys
7 -+ E transformation behavior in a Fe-21Mn alloy with different grain size and a Fe-32Mn-6Si alloy with various degrees of wld rolling is investigated and correlated with damping capacity. Effect of microstructure on damping capacity is discussed on the assumption that the capacity is proportional to volume swept by 7 / e boundaries. 1.INTRODUCTION Fe-Mn based alloys have been well known for s...
متن کامل