Experimental cast titanium alloys containing 20 mass% chromium (Ti-20Cr) show preferable mechanical properties and a good corrosion resistance. This study evaluated the fretting corrosion behavior of Ti-20Cr. Ti-20Cr (n = 4) and commercially pure titanium (CP-Ti, n = 6) disk specimens were used. The fretting corrosion test was performed by electrochemical corrosion at 0.3 V in 0.9% saline solution and mechanical damage using 10 scratching cycles with three different scratching speeds (10-40 mm/s) at 10 N. After testing, the activation peak, repassivation time and surface morphology of each specimen were analyzed. The differences between the results were tested by parametric tests (α = 0.05). The average activation peaks were significantly higher in CP-Ti than in Ti-20Cr (p < 0.01), except at 20 mm/s. In the series of scratching speeds, faster scratching speeds showed higher activation peaks. The maximum activation peaks were also higher in CP-Ti. Slight differences in the repassivation time were observed between the materials at every scratching speed; faster scratching speeds showed shorter repassivation times in both materials (p < 0.05). CP-Ti showed severe damage and significantly higher wear depth than Ti-20Cr (p < 0.05). In conclusion, adding chromium to titanium reduced surface damage and improved the fretting corrosion resistance.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Discoloration of Ti-20Cr alloy in oral environment and its surface characterization.

The objective of this study was to evaluate change in color in experimental titanium-20mass% chromium (Ti-20Cr) alloy in an oral environment. Pure Ti and Ti-6Al-7Nb and Co-29Cr-5Mo alloys, as references to compare change in color, were prepared by casting. The cast specimen was mirror-polished. Each specimen was affixed to a palatal plate and the plate then worn by a volunteer for up to 300 h. ...

متن کامل

Corrosion behavior and surface characterization of Ti-20Cr alloy in a solution containing fluoride.

The purpose of this study was to investigate the correlation between corrosion resistance and surface composition of an experimental Ti-20 mass% Cr casting alloy in a saline solution containing fluoride. The alloy had a greater resistance to corrosion in a fluoride-containing saline solution than did commercially pure titanium. However, with confirmed dissolution of titanium and chromium, it me...

متن کامل

An Experimental Investigation of Fretting Fatigue in Ti-6Al-4V: the Role of Contact Conditions and Microstructure

A systematic investigation of the fretting fatigue behavior of the titanium alloy Ti-6Al-4V in both the mill-annealed (MA) and the solution-treated and overaged (STOA) conditions was carried out. A sphere-on-flat fretting fatigue device was used that facilitated real-time control and monitoring of all the relevant parameters such as the contact geometry, contact (normal and tangential) loads, a...

متن کامل

[Mechanical studies on casting titanium alloy denture base].

The mechanical properties of the Akers type clasp, bar and frame made by the newly developed Ti-20Cr-0.2Si alloy were studied in order to obtain the indices for designing the cast partial denture base. In the case of the clasp, the bending strength of the Ti-20Cr-0.2Si alloy and pure Ti was lower than that of the Co-Cr alloy. The Ti-20Cr-0.2Si alloy and pure Ti may have the same retentive force...

متن کامل

Fretting and Corrosion Damage at the Head-Neck Taper is Reduced with Ceramic Femoral Heads: A Retrieval Study

Introduction: Modular head-neck total hip arthroplasty (THA) offers several benefits for orthopaedic surgeons, including intraoperative flexibility and the ability to change the head at revision surgery [1]. However, modularity at the head-neck taper, especially the use of metallic heads and stems, can lead to fretting and corrosion at the taper junction, leading to metal ions and debris releas...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 10  شماره 

صفحات  -

تاریخ انتشار 2017