Effect of conditioning methods on the microtensile bond strength of phosphate monomer-based cement on zirconia ceramic in dry and aged conditions.

نویسندگان

  • Regina Amaral
  • Mutlu Ozcan
  • Luiz Felipe Valandro
  • Ivan Balducci
  • Marco Antonio Bottino
چکیده

The objective of this study was to evaluate the durability of bond strength between a resin cement and aluminous ceramic submitted to various surface conditioning methods. Twenty-four blocks (5 x 5 x 4 mm(3)) of a glass-infiltrated zirconia-alumina ceramic (In-Ceram Zirconia Classic) were randomly divided into three surface treatment groups: ST1-Air-abrasion with 110-mum Al2O3 particles + silanization; ST2-Laboratory tribochemical silica coating method (110-microm Al2O3, 110-microm silica) (Rocatec) + silanization; ST3-Chairside tribochemical silica coating method (30-microm SiO(x)) (CoJet) + silanization. Each treated ceramic block was placed in its silicone mold with the treated surface exposed. The resin cement (Panavia F) was prepared and injected into the mold over the treated surface. Specimens were sectioned to achieve nontrimmed bar specimens (14 sp/block) that were randomly divided into two conditions: (a) Dry-microtensile test after sectioning; (b) Thermocycling (TC)-(6,000x, 5-55 degrees C) and water storage (150 days). Thus, six experimental groups were obtained (n = 50): Gr1-ST1 + dry; Gr2-ST1 + TC(;) Gr3-ST2 + dry; Gr4-ST2 + TC; Gr5-ST3 + dry; Gr6-ST3 + TC. After microtensile testing, the failure types were noted. ST2 (25.1 +/- 11) and ST3 (24.1 +/- 7.4) presented statistically higher bond strength (MPa) than that of ST1 (17.5 +/- 8) regardless of aging conditions (p < 0.0001). While Gr2 revealed the lowest results (13.3 +/- 6.4), the other groups (21.7 +/- 7.4-25. 9 +/- 9.1) showed statistically no significant differences (two-way ANOVA and Tukey's test, alpha = 0.05). The majority of the failures were mixed (82%) followed by adhesive failures (18%). Gr2 presented significantly higher incidence of ADHESIVE failures (54%) than those of other groups (p = 0.0001). Both laboratory and chairside silica coating plus silanization showed durable bond strength. After aging, air-abrasion with 110-microm Al(2)O(3) + silanization showed the largest decrease indicating that aging is fundamental for bond strength testing for acid-resistant zirconia ceramics in order to estimate their long-term performance in the mouth.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Influence of cement thickness on resin-zirconia microtensile bond strength

PURPOSE The aim of this study was to evaluate the influence of resin cement thickness on the microtensile bond strength between zirconium-oxide ceramic and resin cement. MATERIALS AND METHODS Thirty-two freshly extracted molars were transversely sectioned at the deep dentin level and bonded to air-abraded zirconium oxide ceramic disks. The specimens were divided into 8 groups based on the exp...

متن کامل

Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: the effect of surface conditioning.

OBJECTIVES This study evaluated the effect of three surface conditioning methods on the microtensile bond strength of resin cement to a glass-infiltrated zirconia-reinforced alumina-based core ceramic. METHODS Thirty blocks (5 x 5 x 4 mm) of In-Ceram Zirconia ceramics (In-Ceram Zirconia-INC-ZR, VITA) were fabricated according to the manufacturer's instructions and duplicated in resin composit...

متن کامل

Microtensile Bond Strength of Three Restorative Core Materials with IPS e.max Press Ceramic by Two Resin Cements

Objectives: The aim of this study was to compare the microtensile bond strengths (&micro; TBS) of three core materials with one lithium disilicate reinforced ceramic using two resin cements. Methods: Three core materials (Nulite F&reg; (Biodental Technologies), Filtek Z250&reg; (3M-ESPE), Prettau-Anterior&reg; (Zirkonzhan, Germany)) were prepared as blocks (10&times;10&times;4 mm3) according...

متن کامل

Effect of hydrofluoric acid concentration and etching time on microtensile bond strength of suprinity and enamic CAD/CAM ceramics to resin cement

Introduction: The use of dental ceramics has increased due to their beauty and biocompatibility. The aim of this study was to evaluate the effect of hydrofluoric acid concentration and etching time on microtensile bond strength (μTBS) of the Enamic and Suprinity ceramics. Material & Methods: In this in vitro study, two hydrofluoric acid (HFA) concentrations of 5% (A) and 10% (B) were used at t...

متن کامل

Effect of Laser Irradiation on Bond Strength of Zirconia Ceramic to Self-Adhesive Resin Cement

Background and Aim: Bonding of zirconia to resin cement is challenging, and the zirconia surface requires surface treatment to yield an acceptable bond strength. This study aimed to evaluate the effect of different surface treatments on the bond strength of zirconia to a resin cement. Materials and Methods: In this in-vitro experimental study, 60 zirconia discs measuring 12 mm in diameter an...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of biomedical materials research. Part B, Applied biomaterials

دوره 85 1  شماره 

صفحات  -