A Stretch/Bend Method for In Situ Measurement of the Delamination Toughness of Coatings and Films Attached to Substrates

نویسندگان

  • John W. Hutchinson
  • M. Y. He
  • J. W. Hutchinson
  • A. G. Evans
چکیده

A stretch/bend method for the in situ measurement of the delamination toughness of coatings attached to substrates is described. A beam theory analysis is presented that illustrates the main features of the test. The analysis is general and allows for the presence of residual stress. It reveals that the test produces stable extension of delaminations, rendering it suitable for multiple measurements in a single test. It also provides scaling relations and enables estimates of the loads needed to extend delaminations. Finite element calculations reveal that the beam theory solutions are accurate for slender beams, but overestimate the energy release rate for stubbier configurations and short delaminations. The substantial influence of residual stress on the energy release rate and phase angle is highly dependent on parameters such as the thickness and modulus ratio for the two layers. Its effect must be included to obtain viable measurements of toughness. In a companion paper, the method has been applied to a columnar thermal barrier coating deposited onto a Ni-based super-alloy.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Nonlinear Delamination Mechanics for Thin Films

Delamination of prestressed thin films on thick substrates is analysed accounting for plastic dissipation in either the substrate or film. Emphasis is on large scale yielding wherein the height of the plastic zone at the propagating interface crack tip is comparable to the film thickness. Such conditions are common for both metal and polymer thin films on elastic substrates or for ceramic coati...

متن کامل

Mode II Edge Delamination of Compressed Thin Films

Ceramic coatings deposited on metal substrates generally develop significant compressive stresses when cooled from the temperature at which they are processed as a result of thermal expansion mismatch. One of the main failure modes for these coatings is edge delamination. For an ideally brittle interface, the edge delamination of a compressed thin film involves mode II interface cracking. The c...

متن کامل

Buckling delamination in compressed multilayers on curved substrates with accompanying ridge cracks

Residually compressed films and coatings are susceptible to buckle delamination. The buckles often have linear or telephone cord morphology. When the films are brittle, such buckles are susceptible to the formation of ridge cracks that extend along their length, terminating close to the propagating front. The ridge-cracked buckles are invariably straight-sided (not telephone cord) and differ in...

متن کامل

Numerical Determination of Delamination Onset in Laminated Symmetric DCB Specimen

In this study, a novel numerical method is proposed for determination of mode-I interlaminar fracture toughness, GIc, in multi-directional (MD) double cantilever beam (DCB) specimens using fracture properties of unidirectional DCB specimens. Two factors, β and Dc are defined to minimize the undesirable effects on strain energy release rate. β describes the difference between maximum and average...

متن کامل

Mechanical properties of electrophoretically deposited 45S5 bioglass-graphene oxide composite coatings

Bioglass-graphene oxide composites can be served as a high-potential candidate for biomedical applications due to its specific mechanical properties. In this study, the 45S5 bioactive glass (BG) - graphene oxide (GO) composite containing 2 wt. % GO was coated on titanium alloy via electrophoretic deposition process (EPD). The synthesized GO was incorporated into BG coating to improve the mechan...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2008