The Effect of Hydrofluoric Acid Concentration and Heat on the Bonding to Lithium Disilicate Glass Ceramic.

نویسندگان

  • Daniel Sundfeld
  • Lourenço Correr-Sobrinho
  • Núbia Inocêncya Pavesi Pini
  • Ana Rosa Costa
  • Renato Herman Sundfeld
  • Carmem Silvia Pfeifer
  • Luis Roberto Marcondes Martins
چکیده

The aim of this study was to evaluate the effects of hydrofluoric acid (HF) concentration and previous heat treatment (PHT) on the surface morphology and micro-shear bond strength (mSBS) of a lithium disilicate glass ceramic (EMX) to resin cement. One hundred four EMX specimens were randomly assigned to two groups (n=52) according to the HF concentration: 5% and 10%. A new random distribution was made according to the PHTs (n=13): control (no PHT); previously heated HF (70 °C); previously heated EMX surface (85 °C); the combination of heated HF + heated EMX surface. The etching time was set at 20 s. All EMX blocks were silanated and received a thin layer of an unfilled resin. Five resin cement cylinders were made on each EMX surface using Tygon tubes as matrices, and then stored for 24 h at 37 °C. One random etched EMX sample from each group was analyzed using field-emission scanning electron microscopy (FE-SEM). The data were subjected to two-way ANOVA and multiple comparisons were performed using the Tukey post hoc test (a=0.05). For the control groups, 5% HF showed statistically lower mSBS values when compared to 10% HF (p<0.05). PHT increased the mSBS values for 5% HF, yielding statistically similar results to non-PHT 10% HF (p<0.05). FE-SEM images showed increased glassy matrix removal when PHT was applied to HF 5%, but not to the same degree as for 10% HF. PHT has the potential to improve the bond strength of 5% HF concentration on lithium disilicate glass ceramic.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The effect of silane applied to glass ceramics on surface structure and bonding strength at different temperatures

PURPOSE To evaluate the effect of various surface treatments on the surface structure and shear bond strength (SBS) of different ceramics. MATERIALS AND METHODS 288 specimens (lithium-disilicate, leucite-reinforced, and glass infiltrated zirconia) were first divided into two groups according to the resin cement used, and were later divided into four groups according to the given surface treat...

متن کامل

Effect of Lithium Disilicate Reinforced Liner Treatment on Bond and Fracture Strengths of Bilayered Zirconia All-Ceramic Crown

This study was performed to evaluate the effect of a lithium-disilicate spray-liner application on both the bond strength between zirconia cores and heat-pressed lithium-disilicate glass-ceramic veneers, and the fracture strength of all-ceramic zirconia crowns. A lithium-disilicate reinforced liner was applied on the surface of a zirconia core and lithium-disilicate glass-ceramic was veneered o...

متن کامل

Influence of silane and heated silane on the bond strength of lithium disilicate ceramics - An in vitro study

OBJECTIVES To evaluate the effect of silane application and silane heat treatment on lithium-disilicate ceramic when bonded to composite resin. METHODS Twelve blocks of lithium-disilicate (LD) ceramic were fabricated and bonding surfaces were etched using 9.5% hydrofluoric acid (90 seconds). Three experimental groups resulted from the various surface treatment combinations, which included, no...

متن کامل

Effect of hydrofluoric acid etching duration on the roughness and flexural strength of a lithium disilicate-based glass ceramic.

The aim of this study was to examine the effect of different acid etching times on the surface roughness and flexural strength of a lithium disilicate-based glass ceramic. Ceramic bar-shaped specimens (16 mm x 2 mm x 2 mm) were produced from ceramic blocks. All specimens were polished and sonically cleaned in distilled water. Specimens were randomly divided into 5 groups (n=15). Group A (contro...

متن کامل

Silanization effect on microtensile bond strength of a self-adhesive luting material to a disilicate- based glass ceramic

Introduction: The rehabilitation of teeth by means of ceramic indirect restorations has been widely performed. Previous studies has shown the effectiveness of silane coupling agents on improving the bond strength of the adhesion of resin cements to ceramics; however, some studies question the use of silane. Objective: To evaluate the effect of silane application on the microtensile bond strengt...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Brazilian dental journal

دوره 27 6  شماره 

صفحات  -

تاریخ انتشار 2016